Aluminium salt slag characterization and utilization--a review.

نویسنده

  • P E Tsakiridis
چکیده

Aluminium salt slag (also known as aluminium salt cake), which is produced by the secondary aluminium industry, is formed during aluminium scrap/dross melting and contains 15-30% aluminium oxide, 30-55% sodium chloride, 15-30% potassium chloride, 5-7% metallic aluminium and impurities (carbides, nitrides, sulphides and phosphides). Depending on the raw mix the amount of salt slag produced per tonne of secondary aluminium ranges from 200 to 500 kg. As salt slag has been classified as toxic and hazardous waste, it should be managed in compliance with the current legislation. Its landfill disposal is forbidden in most of the European countries and it should be recycled and processed in a proper way by taking the environmental impact into consideration. This paper presents a review of the aluminium salt slag chemical and mineralogical characteristics, as well as various processes for metal recovery, recycling of sodium and potassium chlorides content back to the smelting process and preparation of value added products from the final non metallic residue.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Utilization of Soil Stabilization with Cement and Copper Slag as Subgrade Materials in Road Embankment Construction

In this study, unconfined compression tests have been conducted to investigate the impacts of copper slag on mechanical characteristics for stabilized cement and un-stabilized soil. Dozens of specimens were prepared at four percentages of cement (i.e. 0%, 2%, 4% and 6%) and five percentages of copper slag (i.e. 0%, 5%, 10%, 15% and 20%) by weight of dry soil. The samples compacted into a cylind...

متن کامل

Arsine Poisoning in a Slag-washing Plant.

An investigation was carried out in an aluminium recovery works after the simultaneous occurrence of haemolytic anaemia in two workers in the slag disposal plant. The first worker was admitted to hospital suffering from nausea, backache, and haematuria. Jaundice developed on the next day. His urine contained protein, urobilin, haemoglobin, and methaemoglobin but no red cells. During the course ...

متن کامل

Secondary aluminium-iron (III) chloride batteries with a low temperature molten salt electrolyte

Secondary aluminium-iron (III) chloride batteries using a low temperature molten salt electrolyte were constructed and tested. Discharge current densities were in the range 5 to 100mA ( ~ 1 to 2 0 m A c m 2 ; ~ C/4 to 5C); charging currents were 5 m A (C/4 toC/2). Utilization of the positive electrode reactant was low due to the discharge rates and loading procedure. The mode for self discharge...

متن کامل

Distribution of trace elements in coal and coal fly ash and their recovery with mineral processing practices: A review

Today coal is among the most important energy sources. In order to meet the world's energy demands, low-calorie lignite with a high ash content is generally used in the large capacity coal-fired thermal power plants. As a result of coal firing, wastes such as fly ash, slag, and flue gas are also produced. Subsequently, toxic trace elements within coal are transferred to wastes such as slag, fl...

متن کامل

Application practice of BOF Slag tailings in steelmaking process

The present paper introduces the steel production and BOF slag processing techniques in Steelmaking Sector of Bayuquan Iron and Steel Subsidiary, Ansteel. The technology of slag tailings utilization has been developed under the consideration of the properties of slag tailing and the characteristics of slag forming in BOF steelmaking operation practice. The processing of the BOF slag includes ho...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of hazardous materials

دوره 217-218  شماره 

صفحات  -

تاریخ انتشار 2012