Graphitic tribological layers in metal-on-metal hip replacements.

نویسندگان

  • Y Liao
  • R Pourzal
  • M A Wimmer
  • J J Jacobs
  • A Fischer
  • L D Marks
چکیده

Arthritis is a leading cause of disability, and when nonoperative methods have failed, a prosthetic implant is a cost-effective and clinically successful treatment. Metal-on-metal replacements are an attractive implant technology, a lower-wear alternative to metal-on-polyethylene devices. Relatively little is known about how sliding occurs in these implants, except that proteins play a critical role and that there is a tribological layer on the metal surface. We report evidence for graphitic material in the tribological layer in metal-on-metal hip replacements retrieved from patients. As graphite is a solid lubricant, its presence helps to explain why these components exhibit low wear and suggests methods of improving their performance; simultaneously, this raises the issue of the physiological effects of graphitic wear debris.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The composition of tribofilms produced on metal-on-metal hip bearings.

Following wear testing in a hip simulator, the bearing surfaces of 36 mm metal on metal total hip replacements showed the formation of tribochemical layers. These layers were investigated in a transmission electron microscope, and analysis was performed using electron energy loss spectroscopy, energy dispersive x-rays and selected area electron diffraction. The tribofilm formed at the edge of t...

متن کامل

CoCrMo metal-on-metal hip replacements.

After the rapid growth in the use of CoCrMo metal-on-metal hip replacements since the second generation was introduced circa 1990, metal-on-metal hip replacements have experienced a sharp decline in the last two years due to biocompatibility issues related to wear and corrosion products. Despite some excellent clinical results, the release of wear and corrosion debris and the adverse response o...

متن کامل

Influence of Bearing Couple, Lubricant and Swing Phase Load Conditions on the Friction of 28mm Hip Replacements

INTRODUCTION The majority of current artificial hip implants use a material combination of ultra-high molecular-weight polyethylene against metal or ceramic. However, it is well documented that the wear debris from these prostheses contributes to osteolysis and ultimate failure of the prosthesis, hence alternative materials have been sought, such as metalon-metal and ceramic-on-ceramic [1]. Mor...

متن کامل

Hard-on-Hard Lubrication in the Artificial Hip under Dynamic Loading Conditions

The tribological performance of an artificial hip joint has a particularly strong influence on its success. The principle causes for failure are adverse short- and long-term reactions to wear debris and high frictional torque in the case of poor lubrication that may cause loosening of the implant. Therefore, using experimental and theoretical approaches models have been developed to evaluate lu...

متن کامل

The clinical performance of metal-on-metal as an articulation surface in total hip replacement.

The metal-on-metal articulations in total hip arthroplasty (THA) were widely used between 1960 and 1975. The McKee-Farrar and other first-generation prostheses failed at a high rate because impingement caused early component loosening. The problem of early component loosening was corrected by improved component design and better manufacturing quality. Second-generation metal-on-metal total hip ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید