Temperature excursions at the pulp-dentin junction during the curing of light-activated dental restorations.

نویسندگان

  • Michael B Jakubinek
  • Catherine O'Neill
  • Chris Felix
  • Richard B Price
  • Mary Anne White
چکیده

OBJECTIVES Excessive heat produced during the curing of light-activated dental restorations may injure the dental pulp. The maximum temperature excursion at the pulp-dentin junction provides a means to assess the risk of thermal injury. In this investigation we develop and evaluate a model to simulate temperature increases during light-curing of dental restorations and use it to investigate the influence of several factors on the maximum temperature excursion along the pulp-dentin junction. METHODS Finite element method modeling, using COMSOL 3.3a, was employed to simulate temperature distributions in a 2D, axisymmetric model tooth. The necessary parameters were determined from a combination of literature reports and our measurements of enthalpy of polymerization, heat capacity, density, thermal conductivity and reflectance for several dental composites. Results of the model were validated using in vitro experiments. RESULTS Comparisons with in vitro experiments indicate that the model provides a good approximation of the actual temperature increases. The intensity of the curing light, the curing time and the enthalpy of polymerization of the resin composite were the most important factors. The composite is a good insulator and the greatest risk occurs when using the light to cure the thin layer of bonding resin or in deep restorations that do not have a liner to act as a thermal barrier. SIGNIFICANCE The results show the importance of considering temperature increases when developing curing protocols. Furthermore, we suggest methods to minimize the temperature increase and hence the risk of thermal injury. The physical properties measured for several commercial composites may be useful in other studies.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Three Light Curing Protocols and Load Cycling on Microleakage of Class V Composite Restorations

  Objective: Different methods have been suggested to overcome the polymerization shrinkage of composite restorations. Changing the light curing protocol to improve polymerization by using new light curing units is among these methods. The new devices are more efficient, portable and durable and produce less heat. This study aimed to assess the marginal microleakage of class V composite restora...

متن کامل

Thermal variations in the pulp chamber associated with composite insertion techniques and light-curing methods.

AIM The aim of this study was to investigate the effect of different incremental insertion techniques, photoactivation, and restorative phases on thermal variations occurring during the polymerization of Filtek Z250 composite resin. METHODS AND MATERIALS The experiment was conducted using 90 bovine incisor teeth. The teeth were randomly assigned to three groups according to the technique used...

متن کامل

Temperature changes under demineralized dentin during polymerization of three resin-based restorative materials using QTH and LED units

OBJECTIVES Light-curing of resin-based materials (RBMs) increases the pulp chamber temperature, with detrimental effects on the vital pulp. This in vitro study compared the temperature rise under demineralized human tooth dentin during light-curing and the degrees of conversion (DCs) of three different RBMs using quartz tungsten halogen (QTH) and light-emitting diode (LED) units (LCUs). MATER...

متن کامل

Temperature rise during photo-polymerization under ceramic restorations.

AIM The aim of this study was to measure the temperature increase induced by various light-curing units during photo-polymerization beneath ceramic restorations. METHODS Three light-curing units were used; a high intensity QTH unit Elipar 2500 and two LED units: Translux Power Blue and Excelled 1400. The 15 ceramic specimens (CEREC Blocks) used in this study were of 2.5 mm thickness, 5 mm wid...

متن کامل

Comparison of the heat generation of light curing units.

AIM The aim of this study was to evaluate the heat generation of three different types of light curing units. METHODS AND MATERIALS Temperature increases were recorded from a distance of 1 mm from a thermocouple to the tip of three different types of light curing units including one quartz-tungsten halogen (QTH), one plasma arc (PAC), and one light emitting diode (LED) unit. An experimental m...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Dental materials : official publication of the Academy of Dental Materials

دوره 24 11  شماره 

صفحات  -