The strength degrading effects of sharp-contact damage are examined for Y-TZP ceramic plates bonded to a plastic substrate. Contacts are made with Vickers and Berkovich diamond indenters at low loads (0.1 N to 100 N) in the ceramic lower surfaces prior to bonding to the substrates. The indentations remain in the subthreshold region, that is, without visible corner radial cracks, over the lower region (< 10 N) of the load range. A concentrated load is then applied sinusoidally to the ceramic upper surface, with the loading axis centered on the subsurface indentation flaw, thereby subjecting the flaw to cyclic tension. Relative to polished surfaces, the indentations diminish the single-cycle strength by an amount that increases with increasing indentation load. The critical number of cycles required to cause failure from the indentation flaws is then measured at specified maximum lower surface tensile stresses. At each indentation load, the strength of the ceramic plates diminishes with increased cycling. The scale of degradation is compared with that from previous studies on Y-TZP surfaces containing larger-scale surface damage: sandblast damage, as used in dental crown preparation; and blunt-contact trauma from a spherical indenter at 3000 N. These other damage modes are shown to be equivalent in their strength-degrading capacity to diamond pyramid indentations in the microscale load range 0.1 N to 1 N, attesting to the highly deleterious nature of sharp particulate contacts. The mechanism of fatigue is considered in terms of microcrack evolution within the indentation damage zone.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fatigue of Yttria-Stabilized Zirconia: II, Crack Propagation, Fatigue Striations, and Short-Crack Behavior

Fatigue crack propagation in 3Y-TZP was investigated using controlled surface flaws. A unique growth law strongly dependent on the maximum stress intensity factor and quadratically dependent on the amplitude of the range of stress intensity factor was established. This growth law was found to apply for both surface flaws and internal flaws and could be used to predict fatigue lifetime. The pres...

متن کامل

Cyclic fatigue resistance of yttria-stabilized tetragonal zirconia polycrystals with hot isostatic press processing.

This study investigated the influence of surface roughness and cyclic loading on fatigue resistance in Y-TZP subjected to hot isostatic pressing (HIP). Fifty Y-TZP cylinders 3.0 mm in diameter were divided into Group A (polished by centerless method; TZP-CP) or Group B (blasted and acid-etched: TZP-SB150E). Twenty five cp-titanium cylinders (Ti-SB150E) were used as a control. Static and cyclic ...

متن کامل

Plasticity 4 nduced Fatigue Damage in Ceria - Stabil

Current studies on the fatigue lifetime of ceramics are mostly focused on the relation between the stress amplitude (or maximum stress) and cycles to failure. For a more compliant and plastic ceramic which has a pronounced nonlinear stress-strain relation, the role of plastic strain in the fatigue damage is investigated for the first time in this study using a 12 mol% Ce-TZP. By testing at diff...

متن کامل

Osseointegration of Zirconia (Y-TZP) Dental Implants: A Histologic, Histomorphometric and Removal Torque Study in the Hip of Sheep

Objectives: The purpose of the present study was to demonstrate the biocompatibility and rigid osseointegration of a zirconia (Y-TZP) dental implant with acid-etched surface. Materials and methods: Eight zirconia (Y-TZP) implants (CeraRoot, Barcelona) were inserted in the hip of an adult sheep. The animal was sacrificed after 2 months. Four implants were used for histology and histomorphometric...

متن کامل

Effect of Alumina Addition to Zirconia Nano-composite on Low Temperature Degradation Process and Biaxial Strength

Ceramic dental materials have been considered as alternatives to metals for dental implants application. In this respect, zirconia tetragonal stabilized with %3 yttrium, is of great importance among the ceramic materials for endosseous dental implant application. Because of its good mechanical properties and color similar to tooth. The aim and novelty of this study was to design and prepare Y-T...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of biomedical materials research. Part B, Applied biomaterials

دوره 72 2  شماره 

صفحات  -

تاریخ انتشار 2005