OBJECTIVES The flexural strengths of veneering ceramics for zirconia were compared. METHODS With 10 different veneering ceramics for zirconia (test group) and three different veneering ceramics for the metal-ceramic technique (control group) three-point flexural strength and biaxial flexural strength according to ISO 6872: 1995 as well as four-point flexural strength according to EN 843-1: 2005 were measured (n=10). Statistical analysis was performed with one-way ANOVA and post hoc Scheffé test (SPSS, p<0.05). RESULTS For the test group, three-point flexural strength ranged between 77.8+/-8.7 and 106.6+/-12.5MPa without any statistically significant differences, biaxial flexural strength between 69.1+/-4.8 and 101.4+/-10.5MPa with three homogeneous groups and four-point flexural strength between 59.5+/-6.2 and 89.2+/-9.5MPa with five homogeneous groups. The control group showed three-point flexural strength values ranging from 93.3+/-13.5 to 149.4+/-20.5MPa, biaxial flexural strength values from 93.4+/-10.0 to 141.2+/-11.6MPa, and four-point flexural strength values from 82.7+/-8.5 to 116.9+/-9.8MPa. In every case, the results of the four-point flexure test were significantly lower than those obtained in the three-point flexure test. The three-point flexural strengths of the test group are similar to those of two ceramics of the control group. The flexural strength of one ceramic of the control group significantly exceeded the strengths of all other ceramics investigated. CONCLUSION Three-point flexural strength values of veneering ceramics for zirconia are similar to those of veneering ceramics for the metal-ceramic technique. The four-point flexure test among all three tests showed highest discrimination between the different ceramic materials.
منابع مشابه
Biaxial flexural strength of bilayered zirconia using various veneering ceramics
PURPOSE The aim of this study was to evaluate the biaxial flexural strength (BFS) of one zirconia-based ceramic used with various veneering ceramics. MATERIALS AND METHODS Zirconia core material (Katana) and five veneering ceramics (Cerabien ZR; CZR, Lava Ceram; LV, Cercon Ceram Kiss; CC, IPS e.max Ceram; EM and VITA VM9; VT) were selected. Using the powder/liquid layering technique, bilayere...
متن کاملInfluence of Veneering Fabrication Techniques and Gas-Phase Fluorination on Bond Strength between Zirconia and Veneering Ceramics.
PURPOSE Porcelain chipping has been one of the main problems of porcelain-fused-to-zirconia restorations. This study evaluates the bond strengths of layered, pressed, and adhesively bonded porcelain to yttria-stabilized zirconia substrates that have undergone traditional preparation or gas-phase fluorination. MATERIALS AND METHODS A three-point bending test was used to evaluate the bond stren...
متن کاملShear bond strength of veneering porcelain to porous zirconia.
In this study, two types of porous zirconia and dense zirconia were used. The flexural strength of non-layered zirconia specimens and those of the layered zirconia specimens with veneering porcelain were examined. Furthermore, the shear bond strength of veneering porcelain to zirconia was examined. The flexural strength of the non-layered specimens was 1,220 MPa for dense zirconia and 220 to 30...
متن کاملEffect of zirconia surface treatments on the shear strength of zirconia/veneering ceramic composites.
Aim of the investigation was to assess the effect of different surface treatments on the bond strength of veneering ceramics to zirconia. In a shear test, the influences of polishing, sandblasting, and silica-coating of the zirconia surface on bonding were assessed with five different veneering ceramics. In addition the effect of liner application was examined. With one veneering ceramic, the i...
متن کاملEffect of Sandblasting Angle and Distance on Biaxial Flexural Strength of Zirconia-based Ceramics.
AIM Surface treatment is necessarily required for bonding of zirconia to the veneering porcelain and luting cements. Sandblasting is the most common and probably the most efficient surface treatment method. Sandblasting roughens the surface and may affect the flexural strength of zirconia. Different sandblasting protocols may yield variable results. This study sought to assess the effect of san...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Journal of dentistry
دوره 36 5 شماره
صفحات -
تاریخ انتشار 2008