Comparative evaluation of fracture resistance of Ceramic Veneer with three different incisal design preparations - An In-vitro Study.

نویسندگان

  • Ajit S Jankar
  • Yogesh Kale
  • Suresh Kangane
  • Anand Ambekar
  • Manish Sinha
  • Sachin Chaware
چکیده

BACKGROUND Ceramic veneer fracture has occurred mainly at the incisal edge of the veneer because of greater stress. This study compares and evaluates the fracture resistance ceramic veneers with three different incisal preparations. MATERIALS & METHODS 15 human permanent maxillary central incisor extracted were selected which were divided into three groups of 5 each having a different Incial design Preparation. Group 1: No Incisal reduction with facio- incisal bevel, Group 2 : 1 mm incisal reduction with butt joint, Group 3 : 1 mm incisal reduction with 1 mm height of Palatal chamfer. It was found that Group III had greater fracture resistance as compared to Group I and Group II. Group I had least fracture resistance as compared to Group II and III. Group II had greater fracture resistance as compared to Group I but less than Group III. RESULTS Ceramic veneer with 1mm incisal reduction with 1mm height of palatal chamfer showed highest fracture resistance as compared to 1mm incisal reduction with butt joint and no incisal reduction with facial-incisal bevel, in order to achieve better esthetic and functional results. CONCLUSION The palatal chamfer margin results in preservation of some peripheral enamel layer, which eliminates the micro leakage at the palatal margin-restoration interface and also effectively counteracting shear stress. This design provides a definite seat for cementation. How to cite the article: Jankar AS, Kale Y, Kangane S, Ambekar A, Sinha M, Chaware S. Comparative evaluation of fracture resistance of Ceramic Veneer with three different incisal design preparations - An In-vitro Study. J Int Oral Health 2014;6(1):48-54.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

تأثیر دو نوع تراش در مقاومت به شکست پرسلن لامینیت ونیر در مقابل نیروهای متناوب

Background and Aim: Because of stable aesthetic and minimum destructive technique, Porcelain laminate veneer has an important role in aesthetic dentistry. But main reason of failure in this treatment is restoration fracture. Therefore tooth preparation have an important role in fracture resistance of porcelain laminate veneer. The aim of this in vitro study was to evaluate the fracture resistan...

متن کامل

A Comparative Evaluation of Shear Bond Strength of Creation Ceramic Veneer to Metal and Zirconia Cores

Abstract Background and Aim: High chipping rates of the veneering porcelain of zirconia ceramic restorations have been reported in clinical studies. Thus, the shear bond strength (SBS) between the zirconia core and veneering porcelain requires investigation. Materials and Methods: In this in-vitro study, at first, using a computer-aided design/computer-aided manufacturing (CAD/CAM) machine, 1...

متن کامل

Comparative evaluation of resistance failure in nonprecious metal-ceramic restoration at the incisal edge with varying thickness under different application of load: an in vitro study.

OBJECTIVE To determine the resistance failure value of nonprecious metal-ceramic restorations at the incisal edge with varying thickness under different application of load. MATERIALS AND METHODS An Ivorian central incisor was prepared to receive metal-ceramic crown, which was further duplicated, invested, casted and 72 metal dies were fabricated in Co-Cr alloy. Metal dies were relieved with ...

متن کامل

Influence of preparation design and ceramic thicknesses on fracture resistance and failure modes of premolar partial coverage restorations.

STATEMENT OF PROBLEM Preparation designs and ceramic thicknesses are key factors for the long-term success of minimally invasive premolar partial coverage restorations. However, only limited information is presently available on this topic. PURPOSE The purpose of this in vitro study was to evaluate the fracture resistance and failure modes of ceramic premolar partial coverage restorations wit...

متن کامل

In vitro effect of fiber reinforcement on fracture resistance of incisal edge composite restorations

Objective: Introduction of fiber-reinforced composites (FRC) greatly enhanced the restoration of fractured anterior teeth. The purpose of this study was to assess the effect of fiber reinforcement on fracture resistance of incisal edge composite restorations of variable thicknesses. Methods: Forty extracted sound human maxillary incisors were divided into four groups of 10. Incisal reduction wa...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of international oral health : JIOH

دوره 6 1  شماره 

صفحات  -

تاریخ انتشار 2014