Surface composition and texture of titanium polished with colloidal silica suspension and chromic oxide slurry.

نویسندگان

  • Awlad Hossain
  • Seigo Okawa
  • Osamu Miyakawa
چکیده

CP titanium was polished with a colloidal silica suspension and chromic oxide slurry under low and high pressures. The polished surfaces were characterized by means of EPMA and XPS. Irrespective of polishing pressure, colloidal silica suspension successfully created a mirror-like surface that was clean at EPMA level. However, XPS detected a small amount of silicon on the outermost surface. On the other hand, chromic oxide slurry under high pressure yielded a very uneven surface with numerous scratches. The EPMA and XPS results suggested the presence of chromium-containing species in the polished surface, which might include hydroxides as well as oxides. In addition, the level of oxygen concentration was noticeably raised, which probably resulted from the increase of surface oxide film thickness or the extension of oxide-to-metal transition zone.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Chromic Oxide Slurry

CP titanium was polished with a colloidal sitica suspension and chromic ox{de slurry under low and high pressures. The polisheti surfaces wer'e characterized by means of EI]MA and XPS. Irrespeetive of polishing pressure, colloidal silica suspension suecessfully created a mirror-Iike surface that was clean at EPMA level, However, XPS detected a small amount of silicon on the outermost surface. O...

متن کامل

Chemical mechanical polishing of titanium with colloidal silica containing hydrogen peroxide--mirror polishing and surface properties.

Chemical mechanical polishing (CMP) of cpTi (Ti) was carried out using two types of slurries, acidic and basic colloidal silica containing H2O2 up to 3 wt%, to obtain flat and mirror-polished surfaces without any contaminated and reacted layers. Polishing behavior and surface properties were investigated using AFM, EPMA, and XPS. Weight loss of Ti polished by CMP using the basic slurry was larg...

متن کامل

Effect of Surface Morphologies on the Isothermal Oxidation Behavior of MCrAlY Coatings Fabricated by High-velocity Oxyfuel Processes

In this study, the effect of surface morphologies on the isothermal oxidation behavior of MCrAlY coatings fabricated by high-velocity oxyfuel (HVOF) processes was investigated. To do so, free standing coatings with as-sprayed and polished surfaces were isothermally oxidized at 1050°C. The thickness of the bond coat was approximately 380μm. The Ra of the as-sprayed and polished surfaces were 6.4...

متن کامل

Preparation and Polishing Properties of Spherical Porous Silica Abrasive

Problem statement: Abrasive is one of key influencing factors on the polished surface quality in Chemical Mechanical Polishing (CMP). Solid abrasives in CMP slurries are easy to cause polishing scratches. It is well known that reducing the hardness of abrasives would improve the polished surface quality. Therefore, the change in structure or shape of the abrasives means a change in polished sur...

متن کامل

Preparation of surface modified magnetic Iron Oxide nanoparticles and study of their colloidal behavior

In this work, we report synthesis of surface modified superparamagnetic iron oxide nanoparticles (SPION) by co-precipitation method using FeSO4.7H2O and Fe2(SO4)3.5H2O as precursors and trisodium citrate dihydrate as surfactant. Surface modification of the as prepared samples was performed in pot by sol-gel precipitation method u...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Dental materials journal

دوره 24 3  شماره 

صفحات  -

تاریخ انتشار 2005