Thin films of porous anodic aluminum oxide (AAO) on tin-doped indium oxide (ITO) substrates were fabricated through evaporation of a 1,000- to 2,000-nm-thick Al, followed by anodization with different durations, electrolytes, and pore widening. A faster method to obtain AAO on ITO substrates has been developed, which with 2.5 vol.% phosphoric acid at a voltage of 195 V at 269 K. It was found that the height of AAO films increased initially and then decreased with the increase of the anodizing time. Especially, the barrier layers can be removed by extending the anodizing duration, which is very useful for obtaining perforation AAO and will broaden the application of AAO on ITO substrates.
منابع مشابه
A Highly Controllable Electrochemical Anodization Process to Fabricate Porous Anodic Aluminum Oxide Membranes.
Due to the broad applications of porous alumina nanostructures, research on fabrication of anodized aluminum oxide (AAO) with nanoporous structure has triggered enormous attention. While fabrication of highly ordered nanoporous AAO with tunable geometric features has been widely reported, it is known that its growth rate can be easily affected by the fluctuation of process conditions such as ac...
متن کاملNanostructured Metallic Surfaces for Biological and Biomedical Applications
Abstract Noble metalllic electrodes, especially, gold, solid gold-amalgam, silver or palladium are very suitable for biological applications in the field of fragment biological samples detection such as microRNA or proteins as disease markers [1, 2]. Various nanostructured surfaces based on metallic nanopillars, nanorods or nanowires are usefull in microdevices . The present works deals with th...
متن کاملبررسی تغییرات پارامترهای ساختاری نانوسیمهای مغناطیسی نیکل بر بازده الکترونهشت
In this work, magnetic Ni nanowire arrays were ac-pulse electrodeposited into the anodic aluminum oxide (AAO) template fabricated by the common two-step anodization technique. The barrier layers at the bottom of the pores were exponentially thinned in a non-equilibrium anodization process to 8, 12, 16 and 20 V. These were fabricated using the constant of 15 mA deposition current, 48 mS off-tim...
متن کاملNanostructuring discotic molecules on ITO support.
Patterning of organic compounds on a nanometer length scale is of great interest for solar applications: defined control over the donor-acceptor interface will allow design of an optimized nano-morphology promoting exciton separation and reducing charge recombination. Herein we present an imprinting technique using anodized alumina oxide (AAO) hard templates as stamps. We show an exact pattern ...
متن کاملIn situ determination of the pore opening point during wet-chemical etching of the barrier layer of porous anodic aluminum oxide: nonuniform impurity distribution in anodic oxide.
Wet-chemical etching of the barrier oxide layer of anodic aluminum oxide (AAO) was systematically investigated by using scanning electron microscopy (SEM), secondary ion mass spectrometry (SIMS), and a newly devised experimental setup that allows accurate in situ determination of the pore opening point during chemical etching of the barrier oxide layer. We found that opening of the barrier oxid...
متن کامل