Metallurgical Analysis of High Pressure Gas Pipelines Rupture

نویسندگان

  • F. Hasan
  • F. Ahmed
چکیده

On 6 July 2004, two parallel-running gas pipelines (18-inch and 24-inch diameters), in the main transmission network of SNGPL (a gas company in Pakistan) were ruptured. The ruptures occurred in the early hours of the morning about 8 miles downstream of the compressor station AC-4. The ruptures were indicated by the increased gas flow at the outlet of AC-4 [1], first at about 0648 hours and then again about 20 minutes later. The gas escaping from the ruptured lines had caught fire, and the flames had also ‘affected’ a third parallel-running pipeline of 30-inch diameter, lying next to the 24-inch line. The metallurgical examination of the two ruptured lines showed that the 24-inch line was ruptured with the help of an explosive device that had been placed on the underside of the pipe. An examination of the 18-inch line showed that this pipe had failed as a result of the heating of the pipe-wall, presumably, by the flame emanating from the 24-inch line. These two observations clearly suggested that the 24-inch line was the first to rupture (by explosives), and the fire following this rupture had heated the 18-inch pipe to a temperature where its yield strength was unable to support the inside gas pressure. The 20 minutes time interval between the two ruptures was obviously the time taken by the 18-inch pipe to be heated upto the level where it started to yield. The 30-inch line lying next to the 24-inch line was affected to the extent that its coating had been burnt-off over a length of about 40-50 feet. However, the pipe did not exhibit any signs of deshaping or deformation what-so-ever. A replica metallographic examination indicated that the microstructure of the pipe was not measurably affected by the heat. It was thus decided not to replace the ‘affected’ part of the 30-inch pipe, but only to re-coat this affected portion.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A Review of Manufacturing Process of Polyethylene Pipe and Connectors for Applying in High-Pressure Natural Gas Pipelines

In this article various pipes used for transporting of gas are introduced and pros and cons of each one are elucidated. The pipes are categorized in three different subgroups including metallic, polymeric and metallic-wire reinforced polymeric pipes. Metallic-wire reinforced polymeric pipes are nominated as the best option for usage in high pressure pipelines transporting natural gas. As a resu...

متن کامل

Research on Leakage Detection and Analysis of Leakage Point in the Gas Pipeline System

Recently, with large-scale use of natural gas and massive constructions of gas pipelines, more and more public concern is focused on pipeline leakage. The leakage caused by holes on gas pipelines generates economic losses to gas companies and causes risks to the environment and sometimes accidents. In order to detect and locate pipeline rupture immediately, the leakage detection method plays a ...

متن کامل

Transient modeling of gas flow in pipelines following catastrophic failure

This paper simulates transient compressible adiabatic gas flows in a long pipeline following a catastrophic failure using an implicit high order finite difference scheme as a discretisation technique for convective terms. A rupture is assumed to be occurred accidentally at a distance from the feeding point of a pipeline where the pipeline being divided into two distinct sections, high and low p...

متن کامل

Oil/Gas Pipeline Leak Inspection and Repair in Underwater Poor Visibility Conditions: Challenges and Perspectives

Mechanical pressure clamps are examples of innovative tools commonly used in the oil and gas industry for arresting leaks from damaged oil and gas pipelines. However, if leaks result from pipeline rupture, clamps are not usually recommended. It is therefore obvious that inspection of the leaking pipeline is very crucial in deciding the strategy for repair. For subsea pipelines where underwater ...

متن کامل

Influence of Pipeline Operating Pressure on Value Setting of Automatic Control Valves at Different Pressure Drop Rates

When a natural gas pipeline ruptures, the adjacent upstream and downstream automatic control valves (ACV) should close quickly to prevent leakage or explosion. The differential pressure set point (DPS) at each valve location is the main criteria for value setting in ACV actions. If the DPS is not properly adjusted, the ACV may mistakenly close or it may not take any actions at a proper ti...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2007