Bacterial penetration of restored cavities using two self-etching bonding systems
نویسندگان
چکیده
OBJECTIVE The aim of this study was to investigate the effects of two bonding systems, with and without antibacterial monomers, on marginal bacterial and dye leakage. MATERIALS AND METHODS Class V cavities were prepared in extracted teeth for a bacterial leakage test, and the teeth were sterilized using a steam autoclave. Four cavities were not restored for the controls, and the other teeth were divided into two groups (n = 16 cavities each): Clearfil Protect Bond group (CPB) and Clearfil SE Bond group (CSE). After application of the bonding agent, the cavities were restored using a composite resin (Clearfil AP-X). The teeth were thermocycled, stored in a broth culture of 1.56 × 108 colony forming units (CFU)/ml of Streptococcus mutans at 37°C for 10 days, and subsequently processed for bacterial staining. Sections from the demineralized teeth were evaluated under a light microscope. In the dye leakage test, the cavities were restored as described in the bacterial penetration test. After thermocycling, the teeth were immersed in 5% basic fuchsin for 24 h, and then divided in half and observed under a stereomicroscope. The data were analyzed using the Kruskal-Wallis and Mann-Whitney U-tests (P = 0.05). RESULTS The bacterial stain was detected at the cavity wall of five cavities in both bonding systems. Additionally, two cavities in the CSE group, one cavity in the CPB group, and all control cavities showed bacterial staining within the cut dentinal tubules. Dye staining at the axial cavity wall was detected in only three of the teeth for both bonding systems. CONCLUSION The bonding systems used in this study provided an acceptable marginal seal to prevent bacterial and dye leakage.
منابع مشابه
Microleakage in Class V Cavities Restored with Sandwich Technique: Self-Etch versus Total-Etch Bonding Systems
Objective: Microleakage has always been a problem in restorative dentistry. To decrease microleakage, modern bonding systems, different application methods and sandwich technique have been recommended. The purpose of this study was to assess the microleakage in class V cavities restored with open sandwich technique using self-etch and total-etch bonding systems. Methods: In this in vitro st...
متن کاملEvaluation of Microleakage of Silorane and Methacrylate Based Composite Materials in Class I Restorations by Using Two Different Bonding Techniques
BACKGROUND To evaluate the microleakage of silorane-based composite material (Filtek P90) with that of two homologous methacrylate-based composites materials (Filtek Z250 and Filtek Z250 XT), by using two different bonding techniques. MATERIALS AND METHODS Sixty extracted human maxillary first premolars prepared for standardized Class I cavities (4 mm × 2 mm × 2 mm) were randomly divided into...
متن کاملتأثیر هیپوکلریت سدیم بر میزان ریزنشت در ترمیمهای کامپوزیت
Statement of Problem: Considering that the role of collagen fibers in dentin adhesion has not been thoroughly established yet, the removal of exposed collagen fibers with a deproteinization agent such as sodium hypochlorite following etching may facilitate access of adhesive resins to a substrate that is more penetrable and less sensitive to water content which in turn would lead to a more dura...
متن کاملبررسی میزان ریزنشت کامپوزیت خود باندشونده WetBond در حفرات کلاس V
Introduction:The self adhesive composite has been introduced for reducing the process of using composite. The new composites can chemically and micromechanily attach to tooth without using bonding. There are no studies that show the traits of these composites. The purpose of this study was to compare the microleakage of a new self-adhesive flowable composite whit usual bonding (excite), and Tet...
متن کاملComparison of Microleakage of Self-etch and Total-etch Bonding Agents in Primary Molar Class II Composite Restorations
Introduction: This study evaluated microleakage of flowable and conventional composite in primary molar class II restorations using self-etch and total-etch bonding agents. Methods: Class II standard cavities were prepared on proximal surface of 48 primary molars. These cavities were restored using GrandioFlow and Grandio composites and Futurabond DC and Solobo...
متن کامل