چکیده

This paper aims to fabricated high quality anodic aluminum oxide (AAO) film by anodization method. AAO pore size, pore density, and film thickness can be controlled in 10~500 nm, 10~10 pore.cm, and 1~100 μm. AAO volume and surface area can be computed based on structural parameters such as thickness, pore size, pore density, and sample size. Base on the thetorical calculation, AAO has 100 μm thickness with 15 nm, 60 nm, and 500 nm pore diameters AAO surface areas are 1225.2 cm, 3204.4 cm, and 549.7 cm, respectively. The large unit surface area which is useful for adsorption application. When AAO adsorbed pH indictor of bromphenol blue presented a sensitive pH detection of solution change. This testing method can further be used for the precise measurement of biotechnology, convenience measurement of industrial engineering. Keywords—AAO, Pore, Surface area, Adsorption, Indicator

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Synthesis of porous CdO sheet-like nanostructure based on soft template model and its application in dye pollutants adsorption

In this work, the synthesis of porous structure of cadmium oxide with multilayered sheet-like morphology in nano-meter size using adipic acid as soft template by solvothermal/thermal decomposition process is reported. Chemical analyses exhibited that the formation of porous sheet-like structure is originated from bidentate coordination mode of adipate units to Cd-center. It was found that the c...

متن کامل

Synthesis of porous CdO sheet-like nanostructure based on soft template model and its application in dye pollutants adsorption

In this work, the synthesis of porous structure of cadmium oxide with multilayered sheet-like morphology in nano-meter size using adipic acid as soft template by solvothermal/thermal decomposition process is reported. Chemical analyses exhibited that the formation of porous sheet-like structure is originated from bidentate coordination mode of adipate units to Cd-center. It was found that the c...

متن کامل

Template Assisted Method for Enhancing the Zeolite’s Ability to Capture Methionine

To investigate template effect on physicochemical properties of zeolite and enhance the molecular sieving properties, adsorption of methionine amino acid was studied by spectroscopic methods. Four zeolites such as methionine templated analcime, methionine templated zeolite P, N, N-dibenzyl N,N,N,N-tetramethylethylenediamine (DBTMED) templated analcime and free template analcime were synthesized...

متن کامل

Kinetic studies of Pb and Ni adsorption onto MCM-41 amine-functionalized nano particle

In the current investigation a novel nano hybrid adsorbent MCM-41/N-(3-trimethoxysilyl)-propyl)diethylenetriamine (MCM-41/TMSPDETA) was prepared and was characterized using DLS (Dynamic Light Scattering), Fourier Transform Infrared (FTIR), X-ray diffraction (XRD), Brunauer–Emmett–Teller (BET) analytical techniques and Transmission electron microscopy (TEM). The synthesized MCM-41/TMSPDETA adsor...

متن کامل

Toward a facile synthesis of spherical sub-micron mesoporous silica: Effect of surfactant concentration

In this paper, a facile method for preparing sub-micron spherical mesoporous silica by the sol-gel process and cationic surfactant cetyltrimethylammonium bromide (CTAB) as a soft template was reported. Moreover, the effect of surfactant concentration on the specific surface area and the total pore volume was investigated. The specific surface area, pore characteristic, morphology, chemical comp...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2012