Strain-based fatigue data for Ti–6Al–4V ELI under fully-reversed and mean strain loads

نویسندگان

  • Patricio E. Carrion
  • Nima Shamsaei
چکیده

This article presents the experimental data supporting the study to obtain the mean strain/stress effects on the fatigue behavior of Ti-6Al-4V ELI. A series of strain-controlled fatigue experiments on Ti-6Al-4V ELI were performed at four strain ratios (-1, -0.5, 0, and 0.5). Two types of data are included for each specimen. These are the hysteresis stress-strain responses for the cycle in a log10 increment, and the maximum and minimum stress-strain responses for each cycle. Fatigue lives are also reported for all the experiments.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Cyclic deformation and fatigue data for Ti–6Al–4V ELI under variable amplitude loading

This article presents the strain-based experimental data for Ti-6Al-4V ELI under non-constant amplitude cyclic loading. Uniaxial strain-controlled fatigue experiments were conducted under three different loading conditions, including two-level block loading (i.e. high-low and low-high), periodic overload, and variable amplitude loading. Tests were performed under fully-reversed, and mean strain...

متن کامل

Data related to cyclic deformation and fatigue behavior of direct laser deposited Ti–6Al–4V with and without heat treatment

Data is presented describing the strain-controlled, fully-reversed uniaxial cyclic deformation and fatigue behavior of Ti-6Al-4V specimens additively manufactured via Laser Engineered Net Shaping (LENS) - a Direct Laser Deposition (DLD) process. The data was collected by performing multiple fatigue tests on specimens with various microstructural states/conditions, i.e. in their 'as-built', anne...

متن کامل

Microstructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation

Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...

متن کامل

Microstructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation

Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...

متن کامل

An Experimental Investigation of Fretting Fatigue in Ti-6Al-4V: the Role of Contact Conditions and Microstructure

A systematic investigation of the fretting fatigue behavior of the titanium alloy Ti-6Al-4V in both the mill-annealed (MA) and the solution-treated and overaged (STOA) conditions was carried out. A sphere-on-flat fretting fatigue device was used that facilitated real-time control and monitoring of all the relevant parameters such as the contact geometry, contact (normal and tangential) loads, a...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 7  شماره 

صفحات  -

تاریخ انتشار 2016