Multi-Scale Effects in the Strength of Ceramics.

نویسنده

  • Robert F Cook
چکیده

Multiple length-scale effects are demonstrated in indentation-strength measurements of a range of ceramic materials under inert and reactive conditions. Meso-scale effects associated with flaw disruption by lateral cracking at large indentation loads are shown to increase strengths above the ideal indentation response. Micro-scale effects associated with toughening by microstructural restraints at small indentation loads are shown to decrease strengths below the ideal response. A combined meso-micro-scale analysis is developed that describes ceramic inert strength behaviors over the complete indentation flaw size range. Nano-scale effects associated with chemical equilibria and crack velocity thresholds are shown to lead to invariant minimum strengths at slow applied stressing rates under reactive conditions. A combined meso-micro-nano-scale analysis is developed that describes the full range of reactive and inert strength behaviors as a function of indentation load and applied stressing rate. Applications of the multi-scale analysis are demonstrated for materials design, materials selection, toughness determination, crack velocity determination, bond-rupture parameter determination, and prediction of reactive strengths. The measurements and analysis provide strong support for the existence of sharp crack tips in ceramics such that the nano-scale mechanisms of discrete bond rupture are separate from the larger scale crack driving force mechanics characterized by continuum-based stress-intensity factors.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

An investigation on Mechanical Properties of Apatite-Wollastonite-Diopside Glass-Ceramics Composites

Apatite-wollastonite (A-W)-phlogopite glass-ceramic is considered to be difficult to resorb, but often, it has been incorporated in particulate form to create new bioactive composites for potential maxillofacial applications. With various compositions, the present work has attempted to prepare apatite-wollastonite (A-W)-phlogopite glass ceramic composites, by applying sintering. Here, three-poi...

متن کامل

Effect of hydrofluoric acid concentration and etching time on microtensile bond strength of suprinity and enamic CAD/CAM ceramics to resin cement

Introduction: The use of dental ceramics has increased due to their beauty and biocompatibility. The aim of this study was to evaluate the effect of hydrofluoric acid concentration and etching time on microtensile bond strength (μTBS) of the Enamic and Suprinity ceramics. Material & Methods: In this in vitro study, two hydrofluoric acid (HFA) concentrations of 5% (A) and 10% (B) were used at t...

متن کامل

Effect of Thermal and Mechanical Aging on Flexural Strength of Zirkonzahn and Mamut Zirconia Ceramics

  Objective: Despite the high strength of zirconia restorations, aging in the oral environment and masticatory loading may result in transformation of tetragonal to monoclinic phase and decrease their strength. Statements in this regard are controversial. This study sought to compare the flexural strength (FS) of Zirkonzahn (ZirkonZahn, Cercon, Ceramill) and Mamut (Dubai Medical Equipment LLC, ...

متن کامل

Investigation of the Physical and Mechanical Properties of Silicon Carbide Prepared on an Industrial Scale

In this study, an industrial polycrystalline SiC tile was successfully sintered by pressureless sintering at 2150°C for 1 hour. The physical and mechanical properties of silicon carbide including density, hardness, bending strength, and fracture toughness were evaluated. The results indicated that the mentioned properties were 3.08 g.cm-3, 2503 HV0, 249.3 MPa, and 1.23 MPam0.5</...

متن کامل

مقایسه استحکام باند ریزبرشی سرامیک‌های Cercon و Zirkonzahn با دو نوع سمان رزینی

  Background and Aims: Nowadays, the application of all ceramic restorations are being raised, because of their physical characteristics, such as translucency and good appearance. Numerous researchers investigated the impact of surface treatments on the bond strength of zirconia ceramic with resin cements. The aim of this study was to compare the microshear bond strength of Cercon and Zirkonzah...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of the American Ceramic Society. American Ceramic Society

دوره 98 10  شماره 

صفحات  -

تاریخ انتشار 2015