STATEMENT OF PROBLEM Computer-aided design/computer-aided manufacturing (CAD/CAM) titanium ceramic restorations were developed with the potential for replacing expensive, high noble metal ceramic restorations. However, there is a lack of information about the clinical performance of CAD/CAM titanium ceramic single crowns. PURPOSE The purpose of this study was to evaluate CAD/CAM titanium ceramic single crowns after 3 years in function. MATERIAL AND METHODS A total of 41 crowns were fabricated for 21 patients. The titanium copings were CAD/CAM milled (Everest CAD/CAM system) with an even thickness of 0.5 mm, and low-fusing veneering porcelain (Vita Titanium Porcelain) was added incrementally. The crowns were cemented using zinc phosphate cement after confirming that there were no mechanical and biological complications. The patients were recalled at 12, 24, and 36 months after cementation to examine the presence of any complications and measure periodontal parameters such as probing depth (PD), bleeding on probing (BOP), and plaque index (PI). The success and survival rates were estimated using the Kaplan-Meier analysis. RESULTS The success rate of CAD/CAM titanium ceramic crowns with regard to mechanical complications was 82.3% (95% confidence interval: 71.2% to 95.1%). The cumulative survival rate of the crowns was 94.9% (95% confidence interval: 88.3% to 100%) after 3 years. No biological complications were observed. At the end of the follow up, PD was 2.93 mm, percentile of surface with BOP was 29.2, and PI was 0.31. CONCLUSIONS The clinical performances of the CAD/CAM titanium ceramic crowns for 3 years were acceptable, with no biologic complications and a high cumulative survival rate.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

CAD/CAM-titanium-ceramic single crowns with non-anatomic coping-design. A six-year follow-up study

Objectives Due to the increasing price of gold CAD/CAM titanium-ceramic restorations were developed to give alternative to the established metal-ceramic restorations with a high gold content. Despite the advantages of excellent biocompatibility, high corrosion resistance and appropriate strength titanium has made the casting process difficult caused by the high affinity of molten titanium to in...

متن کامل

The Effect of Different Finishing Lines on the Marginal Fitness of Full Contour Zirconia and Glass Ceramic CAD/CAM Crowns (An in-vitro study)

Purpose: The aim of this study was to evaluate the effect of two gingival finishing lines (90° shoulder and deep chamfer) on the marginal fitness of two types of full anatomic all-ceramic crowns; zirconia crowns (Zikonzhan) and glass ceramic crowns (IPS e-max CAD) milled with CAD/CAM system. Materials and Methods: Two dentoform teeth of left maxillary first molar were prepared with chamfer fini...

متن کامل

CAD/CAM to fabricate ceramic implant abutments and crowns: a preliminary in vitro study.

BACKGROUND This study evaluated the feasibility of fabricating implant abutments and crowns from pre-sintered feldspathic porcelain blocks using the chair-side CAD/CAM, CEREC3D((R)) system. METHODS Thirty-two implant analogues were divided into two groups. In the control group, prefabricated machined anatomical titanium (Ti) abutments were screw-retained to the analogues. In the test group, m...

متن کامل

Clinical Marginal and Internal Adaptation of Maxillary Anterior Single All-Ceramic Crowns and 2-year Randomized Controlled Clinical Trial.

PURPOSE The aims of this randomized-controlled clinical trial were to compare marginal and internal adaptation of all-ceramic crowns fabricated with CAD/CAM and heat-pressed (HP) techniques before luting and to evaluate the clinical outcomes at baseline and at 6, 12, and 24 months after luting. MATERIALS AND METHODS Fifteen CAD/CAM (CC) and 15 HP all-ceramic crowns were placed in 15 patients....

متن کامل

Comparative fracture strength analysis of Lava and Digident CAD/CAM zirconia ceramic crowns

PURPOSE All-ceramic crowns are subject to fracture during function. To minimize this common clinical complication, zirconium oxide has been used as the framework for all-ceramic crowns. The aim of this study was to compare the fracture strengths of two computer-aided design/computer-aided manufacturing (CAD/CAM) zirconia crown systems: Lava and Digident. MATERIALS AND METHODS Twenty Lava CAD/...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • The Journal of prosthetic dentistry

دوره 102 5  شماره 

صفحات  -

تاریخ انتشار 2009