Effect of Multiple Adhesive Coating on Microshear Bond Strength to Primary Tooth Dentin

نویسندگان

  • Beheshteh Malekafzali
  • Amir Ghasemi
  • Hassan Torabzadeh
  • Reza Hamedani
  • Nekoo Tadayon
چکیده

OBJECTIVE Multiple adhesive coating is a controversial topic, especially in primary dentition that should be clarified. We evaluated the effect of multiple consecutive adhesive resin coatings on the microshear bond strength (μSBS) of composite resin to primary tooth dentin utilizing a filled (Adper Single Bond Plus) and an unfilled (Adper Single Bond) adhesive resin. MATERIALS AND METHODS Thirty extracted primary canines were randomly allocated into two groups based on the adhesive used. Dentin occlusal surfaces were exposed and further polished on 400, 600 and 800-grit silicon-carbide paper. The surfaces were divided into two halves in the labial-lingual orientation. After etching, the adhesives were used either in double coats, or four coats on the halves of the same tooth followed by air evaporation for each layer and finally light curing. Cylinders of composite were bonded to the dentin surfaces. After 24 h shear bond testing was evaluated by Bisco tensile tester. ANOVA, Student t test and paired t test were used for statistical analysis. RESULTS The mean (standard deviation) for double coats or four coats in single bond were 31.99 (2.94) and 30.25 (2.69), while they were 29.18 (3.35) and 31.26 (2.07) in single bond plus, respectively. No significant differences were found between the double coated specimens and those receiving four coatings with both adhesives (p>0.05). Micro SBS values of Single Bond double coated specimens were significantly higher than Single Bond Plus (p=0.02). In four-coated specimens, there were no significant differences between Single Bond and Single Bond Plus (p=0.26). CONCLUSION Applying four coats of adhesive did not improve the μSBS to primary tooth dentin.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

بررسی اثر تعداد لایه‌های ادهزیو بر استحکام باند ریز برشی و ریز سختی سطح باند شده عاج پس از کاربرد چهار نوع ادهزیو

Background and Aims: In this in-vitro study, the effect of multiple adhesive coating on the microshear bond strength of composite to dentin and surface microhardness of dentin after treatment with four adhesives (One Step Plus, One Step, Single Bond, Single Bond 2) were evaluated. Materials and Methods: One hundred intact human molars were cut to obtain disks of dentin having 2 mm thickness. F...

متن کامل

Effect of adhesive layers on microshear bond strength of nanocomposite resin to dentin

BACKGROUND Bond strength of adhesive layer can absorb unwanted stresses of polymerization shrinkage in composite resin restorations; increased microshear bond strength can prevent failure of restoration materials, the purpose of this study was to evaluate the effect of adhesive layers on microshear bond strength of nanocomposite resin to dentin. MATERIAL AND METHODS Two different types of adh...

متن کامل

Effect of two microshear test devices on bond strength and fracture pattern in primary teeth.

This in vitro study evaluated the influence of two devices for application of shear load in microshear tests on bond strength and fracture pattern of primary enamel and dentin. Eighty primary molars were selected and flat enamel (40 teeth sectioned mesio-distally) and dentin (40 teeth sectioned transversally) surfaces were obtained. Both surfaces were polished to standardize the smear layer. Tw...

متن کامل

Microshear bond strength of Nano-Bond adhesive containing nanosized aluminum trioxide particles

OBJECTIVES The present study was conducted to evaluate the effect of nanosized aluminum trioxide (Al2O3) particles when added to the Nano-Bond adhesive system and its effect on the microshear bond strength of nanocomposite resin to dentin. MATERIALS AND METHODS A newly developed adhesive (Nano-Bond) and one type of light-cured resin restorative material (nanocomposite resin) were used in this...

متن کامل

Microshear Bond Strength of Glass Ionomer to Primary Dentin following Surface Treatment by Bur and Er,Cr:YSGG Laser

Background and Aim: Er,Cr:YSGG laser irradiation has been suggested as an effective method of cavity preparation and surface treatment to enhance the bond strength. The aim of this study was to assess the microshear bond strength of Fuji II LC glass ionomer (GI) cement to primary dentin following bur preparation and Er,Cr:YSGG irradiation. Materials and Methods: This in vitro, experimental stu...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 10  شماره 

صفحات  -

تاریخ انتشار 2013