As an ideal anode material, silicon has the highest lithium-ion capacity in theory, but the broader application is limited by the huge volumetric strain caused by lithium insertion and extraction. To better understand the physical process and to resolve the related reliability issue, enormous efforts have been made. Recent experiments observed sharp reaction fronts in both crystalline and amorphous silicon during the first lithiation halfcycle. Such a concentration profile indicates that the process is likely to be reaction limited. Based on this postulation, a phase-field model is developed and implemented into a finite-element code to simulate the coupled large inelastic deformation and motion of the reaction front in a silicon electrode. In contrast to most existing models, the model treats both volumetric and deviatoric inelastic deformation in silicon as a direct consequence of the lithiation at the reaction front. The amount of deviatoric deformation is determined by using the recently developed kinetic model of stress-induced anisotropic reaction. By considering the role of stress in the lithiation process, this model successfully recovers the self-limiting phenomenon of silicon electrodes, and relates it to the local geometry of electrodes. The model is also used to evaluate the energy-release rate of the surface crack on a spherical electrode, and the result suggests a critical size of silicon nanoparticles to avert fracture. As examples, the morphology evolution of a silicon disk and a Si nanowire during lithiation are also investigated. & 2016 Elsevier Ltd. All rights reserved.
منابع مشابه
Synthesis of Three - Dimensional Mesoporous Silicon from Rice Husk via SHS Route
Silicon nanoparticles are the focus of attention thanks to their potentialities in advanced applications such as new batteries, photovoltaic cells and so on. The need to porous silicon is thus rising and will follow the same trend. In this work, highly porous nanostructured silicon is synthesized via Self-propagating high-temperature synthesis (SHS) route. Microstructural and phase analyses sho...
متن کاملKinetics of initial lithiation of crystalline silicon electrodes of lithium-ion batteries.
Electrochemical experiments were conducted on {100}, {110}, and {111} silicon wafers to characterize the kinetics of the initial lithiation of crystalline Si electrodes. Under constant current conditions, we observed constant cell potentials for all orientations, indicating the existence of a phase boundary that separates crystalline silicon from the amorphous lithiated phase. For a given poten...
متن کاملOrientation-dependent interfacial mobility governs the anisotropic swelling in lithiated silicon nanowires.
Recent independent experiments demonstrated that the lithiation-induced volume expansion in silicon nanowires, nanopillars, and microslabs is highly anisotropic, with predominant expansion along the <110> direction but negligibly small expansion along the <111> direction. The origin of such anisotropic behavior remains elusive. Here, we develop a chemomechanical model to study the phase evoluti...
متن کاملTwo-phase electrochemical lithiation in amorphous silicon.
Lithium-ion batteries have revolutionized portable electronics and will be a key to electrifying transport vehicles and delivering renewable electricity. Amorphous silicon (a-Si) is being intensively studied as a high-capacity anode material for next-generation lithium-ion batteries. Its lithiation has been widely thought to occur through a single-phase mechanism with gentle Li profiles, thus o...
متن کاملReaction Front Evolution during Electrochemical Lithiation of Crystalline Silicon Nanopillars
Silicon is one of the most promising anode materials for use in rechargeable lithium-ion batteries due to its high theoretical specific capacity of 4200 mAhg 1 and low cost. However, this high lithium storage capacity results in enormous volume expansion and contraction during electrochemical lithiation and delithiation, which can induce mechanical fracture and severe capacity fading. Recently,...