Bleaching of kaolins and clays by chlorination of iron and titanium

نویسندگان

  • J. A. González
  • M. del C. Ruiz
چکیده

The quality of the clays and over all kaolin is measured in function of iron content, since this element gives an undesirable reddish color to this type of minerals. The use of chlorination for iron and titanium removal from different clay and kaolin minerals, used in Argentinian ceramic industry, has been investigated to establish reaction mechanisms, precautions and optimal conditions to bleach the clays. The method consists of the calcinations of the pellets in a flow of chlorine gas at temperatures between 700 and 950 °C, to remove the iron and the titanium by volatilization of the respective chlorides. Isothermal and non-isothermal chlorination assays were made and the effects of the temperature, reaction time, and carbon content in the sample over the bleach of the minerals and the phase transformations suffered by these minerals during the chlorination step were investigated. The removed amounts of iron and titanium were determined by X-ray fluorescence, the phase transformations were followed by X-ray diffraction and the samples' bleaching was established making an analysis of the space of the color by the spectrophofotometric method CIELAB. Also, a thermodynamic analysis of the system using HSC Chemistry for Windows software was made. The experimental results show that for red clay with high colloidal iron content, the optimum working temperature for the iron quantitative removal, without aluminium loss, is close to 850 °C, in controlled atmosphere free of O2 and H2O; lower temperatures require long reaction times. The extraction of titanium is not quantitatively achieved, as that of iron, even for long reaction times, because this element is present in different structures, with the consequent variation of its reactivity. The content of carbon and organic matter in the clays, in the case of the San Luis red clay, is enough for extraction improvement. However, the optimum concentration of carbon can vary depending on the type of clay and the amount of Fe2O3 in the mineral. The formation of phases such as α-Al2O3, a product of chlorination, increases the piece hardness. The methodology used in this work allows for obtaining a great improvement in the color of the final product of the firing, achieving ceramic materials with notable whiteness, even with red clays. © 2006 Elsevier B.V. All rights reserved.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Phase Transformations in Clays and Kaolins Produced by Thermal Treatment in Chlorine and Air Atmospheres

−A study of the phase transformations generated by chlorine during the calcination of clays and kaolins is presented. The original samples and residues of the thermal treatment carried out in air and chlorine atmospheres are analyzed at different calcination times and temperatures. Sample characterization was performed by X-ray diffraction (XRD), scanning electron microscopy (SEM) and Xray micr...

متن کامل

Iron Removal from Kaolins by Bacterial Leaching

Weathering of rocks generated large volumes of kaolin clays, quartz sands and micas, as well as other minerals, especially iron and titanium oxides. Kaolin is an economically important raw material often used in wide variety of ceramic applications, from high quality tableware and sanitaryware to electrical porcelain, tiles and glasses. There are some less common uses including glass fibre, whi...

متن کامل

Production of titanium tetrachloride (TiCl4) from titanium ores: A review

Titanium (Ti) is the ninth most abundant element on earth. The titanium mineral ores are widely distributed in different parts of the world. The two main ores of titanium include rutile (TiO2) and ilmenite (FeO.TiO2). It is aimed to provide the readers with an insight to the main processes currently employed to extract and recover titanium tetrachloride (TiCl4) from different titanium ores. Due...

متن کامل

Reaction-Mediator-Based Chlorination for the Recycling of Titanium Metal Scrap Utilizing Chloride Waste

In this study, a novel chlorination technique for metallic titanium (Ti) was devised in order to establish a recycling process that uses both Ti metal scrap and iron chloride (FeClx) waste, and its feasibility was demonstrated. Direct reaction between Ti and FeClx has drawbacks such as slow kinetics of Ti chlorination and high volatilization of FeClx. To overcome these, the authors proposed a c...

متن کامل

Investigating the Effect of Titanium Addition on the Microstructure and Mechanical Properties of Ni-Hard 4 Cast Iron

Ni-Hard4 white cast iron is excellent wear resistant material and has been widely used in wearaffected equipment operated under extreme conditions, such as in mineral processing, cement, copper and iron manufacturing. In this study the effect of titanium addition (1.2, 0.7 and 0.2 wt.%) to the Ni-hard 4 cast iron with the nominal composition of Si= 1.5%, Mn=0.5%, C=3%, P=0.05%, S= 0.05%, Mo= 0....

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2006