Electric charging/discharging characteristics of super capacitor, using de-alloying and anodic oxidized Ti-Ni-Si amorphous alloy ribbons

نویسندگان

  • Mikio Fukuhara
  • Kazuyuki Sugawara
چکیده

Charging/discharging behaviors of de-alloyed and anodic oxidized Ti-Ni-Si amorphous alloy ribbons were measured as a function of current between 10 pA and 100 mA, using galvanostatic charge/discharging method. In sharp contrast to conventional electric double layer capacitor (EDLC), discharging behaviors for voltage under constant currents of 1, 10 and 100 mA after 1.8 ks charging at 100 mA show parabolic decrease, demonstrating direct electric storage without solvents. The supercapacitors, devices that store electric charge on their amorphous TiO2-x surfaces that contain many 70-nm sized cavities, show the Ragone plot which locates at lower energy density region near the 2nd cells, and RC constant of 800 s (at 1 mHz), which is 157,000 times larger than that (5 ms) in EDLC.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Ni on Amorphization of Ti-Cu-Ni Ternary alloys Prepared by Mechanical alloying

Amorphous alloys has been taken into consideration because of their unique properties and are nominated as the future engineering materials. In this research, the effect of Ni and milling time on amorphization process and thermal stability of Ti50Cu50-xNix(x=10, 15, 25 at%) alloy system were investigated. The evolution of amorphization during milling, thermal stability and subsequent heat treat...

متن کامل

1 Layout

Mechanical alloying of Ti-Si and NiTi was performed by high-energy ball milling at ambient temperature. The structural and compositional evolutions during mechanical alloying were investigated. Results showed that the crystallite size of mechanically alloyed Ti-Si and Ni-Ti powders decreased with increasing milling time and the steady-state crystallite size was approximately 10 nm. The mechanic...

متن کامل

ارزیابی ریزساختاری آلیاژ Ni-Nb-Si در حین فرایند آلیاژسازی مکانیکی

In the present study, the mechanical alloying process was used to produce the Ni-Nb-Si amorphous alloy. X-ray diffraction (XRD)analysis and high-resolution transmission electron microscopy (HRTEM) were used to approve the amorphous phase formation after 12 hours of mechanical alloying. The results obtained from the SEM morphological images of powder particles during mechanical alloying showed t...

متن کامل

Three-dimensional AlZnO/Al2O3/AlZnO nanocapacitor arrays on Si substrate for energy storage

High density three-dimensional AZO/Al2O3/AZO nanocapacitor arrays have been fabricated for energy storage applications. Using atomic layer deposition technique, the stack of AZO/Al2O3/AZO has been grown in the porous anodic alumina template which is directly formed on the Si substrate. The fabricated capacitor shows a high capacitance density of 15.3 fF/μm2 at 100 kHz, which is nearly 2.5 times...

متن کامل

Synthesis of Nanostructure Ti-45Al-5Cr Alloy by Mechanical Alloying and Study the Effect of Cr Addition on Microstructure of TiAl Alloy

In this work, mechanical alloying was employed to produce Ti-50Al and Ti-45Al-5Cr (at%) alloys. Alloying was performed in a planetary mill and the alloying time varying from 5 to 70h. Characterization of the powder mixture was performed by X-ray diffraction (XRD), SEM analyses and DTA test, during mechanical alloying and after annealing at 1100°c in vacuum oven. The results showed, after 50h of...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 9  شماره 

صفحات  -

تاریخ انتشار 2014