Indentation cracks on ceramics are frequently used not only for the semi-empirical determination of the fracture toughness KIC but also as a method for generating semielliptical surface cracks to be used in as starting cracks in fracture and fatigue studies. Tetragonal zirconia stabilized with 3 % mol of yttria (3Y-TZP) is a biocompatible ceramic with good mechanical properties which is used in dental and femoral prostheses applications. Additionally, 3Y-TZP is susceptible to low temperature degradation in which a hydrothermal environment induces a phase transformation of the exposed surface. In the present work, this degradation susceptibility of 3Y-TZP has been used to reveal indentation crack profiles on specimens which were tested by flexural bending afterwards. Different types of 3Y-TZP were considered which presented different degrees of susceptibility to hydrothermal degradation. It is shown that these cracks are clearly decorated by the water vapour which make them easily revealed on the fracture surfaces. An exposition of few hours in autoclave is sufficient for revealing the indentation cracks on the fracture surface without affecting the fracture load of the specimens. Therefore, the method can be applied to visualize with precision the geometry of indentation cracks which are used to determine the fracture toughness. PALABRAS CLAVE: Cerámicas, Resistencia, Biomateriales
منابع مشابه
Low-temperature degradation of different zirconia ceramics for dental applications.
The aim of this investigation was to determine the influence of simulated ageing on the tetragonal-to-monoclinic phase transformation and on the flexural strength of a 3Y-TZP ceramic, compared to alumina toughened zirconia (ATZ) and ceria-stabilized zirconia (12Ce-TZP). Standardized disc specimens of each material were hydrothermally aged in steam at 134°C and 3bar for 0, 16, 32, 64 or 128h. Th...
متن کاملStability of Nanocrystalline Spark Plasma Sintered 3Y-TZP
Spark plasma sintered 3Y-TZP has been investigated with respect to hydrothermal ageing and grinding. The sintering was performed between the temperatures of 1,100 and 1,600 °C for a soaking time of 5 minutes and the resulting materials were obtained with grain sizes between 65 to 800 nm and relative densities between 88.5 to 98.8%. Experiments on hydrothermal ageing in water vapour at 131 °C, 2...
متن کاملDetermination of the Intrinsic Fracture Toughness from the Cod Analysis of Indentation Cracks in Spark Plasma Sintered 3y-tzp Reinforced with Mwcnt
The indentation method has been widely used to measure the fracture toughness in fragile materials due to its simplicity and that only needs of a small sample. However, it is well known that the fracture toughness values obtained by indentation methods can be substantially different from the values obtained from more rigorous methods which are based on a precise knowledge of all parameters invo...
متن کاملHighly-translucent, strong and aging-resistant 3Y-TZP ceramics for dental restoration by grain boundary segregation.
Latest trends in dental restorative ceramics involve the development of full-contour 3Y-TZP ceramics which can avoid chipping of veneering porcelains. Among the challenges are the low translucency and the hydrothermal stability of 3Y-TZP ceramics. In this work, different trivalent oxides (Al2O3, Sc2O3, Nd2O3 and La2O3) were selected to dope 3Y-TZP ceramics. Results show that dopant segregation ...
متن کاملEffect of different surface treatments on the hydrothermal degradation of a 3Y-TZP ceramic for dental implants.
OBJECTIVES Implant surface modifications are intended to enhance bone integration. The objective of this study was to assess the effect of different surface treatments on the resistance to hydrothermal degradation, hardness and elastic modulus of a 3Y-TZP ceramic used for dental implants. METHODS Samples grouped according to their surface morphologies (AS, as-sintered; C, coated; P, dry-polis...