The effect of different beverages on acrylic resin denture teeth color degradation is evaluated. Ten acrylic resin denture teeth brands were evaluated: Art Plus (AP), Biolux (BX), Biotone IPN (BI), Magister (MG), Mondial 6 (MD), Premium 6 (PR), SR Vivodent PE (SR), Trilux (TR), Trubyte Biotone (TB), and Vipi Dent Plus (VP). Teeth were immersed in staining solutions (coffee, cola, and orange juice) or artificial saliva (control) (n=6) for 1, 7, 15, or 30 days. Specimen colors were evaluated spectrophotometrically based on the Commission Internationale d'Eclairage L*a*b* system. Color differences (ΔE) were calculated between the baseline and post-staining results. Data were evaluated by analysis of variance and Tukey test (α = 0.05). BI (1.82 ± 0.95) and TR (1.78 ± 0.72) teeth exhibited the greatest ΔE values, while BX (0.88 ± 0.43) and MD (1.09 ± 0.44) teeth were the lowest, regardless of solution and measurement period, and were different from BI and TR teeth (P < 0.05). Cola and coffee promoted higher denture teeth color alterations than orange juice and saliva (P < 0.05). Saliva generated the lowest denture teeth color alterations. Greater immersion times caused higher denture teeth color changes. The lifespan of removable dentures and the aesthetic satisfaction of several edentulous patients may be increased with the use of stain-resistant artificial denture teeth.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Bond Strength of Repaired Acrylic Denture Teeth Using Visible Light Cure Composite Resin

BACKGROUND Although bonding to denture teeth after surface treatment with chemical agents is desirable, there is little information on the use of Visible Light Cure composite resin (VLC) as bonding denture materials. OBJECTIVES To determine the effect of various surface treatments on shear bond strength between Visible Light Cure composite resin and the acrylic denture teeth interface. METH...

متن کامل

مقایسه استحکام باند دندان‌های کامپوزیتی و آکریلی به آکریل‌های بیس دنچر گرماپخت و خود به خود پلیمریزه شونده

Background and Aims: Failure of bonding between artificial teeth and denture base material is a considerable problem for patients who wear dentures. Because of the cost of denture repair and the expensive price of foreign artificial teeth, this study was designed to compare the bond strength of composite and acrylic artificial teeth with heat-cured and auto-polymerized denture base resins.Mater...

متن کامل

مقایسه مقاومت به سایش سه نوع دندان مصنوعی کامپوزیتی با یک نمونه از دندان‌های مصنوعی آکریلی

Background and Aims: Wear resistance of artificial teeth has an important role in denture longevity. The purpose of this in vitro study was to evaluate the wear resistance of three types of composite resin denture teeth with that of acrylic resin. Materials and Methods: In this study, four types of artificial teeth, including 3 types of composite artificial teeth (Ivoclar, Apple and Yamahachit...

متن کامل

Comparative Evaluation of Bond Strength of Surface-treated and Surface-modified Anterior Acrylic Teeth

Harold Vernon first introduced acrylic polymers as denture base materials in 1937. A survey showed that 33% of denture repairs were to restore debonded teeth.1 Factors that affect the bonding of acrylic resin teeth to the denture base are dewaxing procedures, residual wax on ridge laps of teeth,2 and careless application separating media like sodium alginate to the teeth, leading to contaminati...

متن کامل

Evaluation of the Effect of 2 Flask Investment Materials on Color Stability of 5 Brands of Denture Teeth

Introduction: The purpose of this study was to investigate the effect of flask investment materials on the color changes of different brands of resin denture teeth. Methods: Resin denture teeth (560) were divided into 2 groups according to the materials used for flask investment (silicone or gypsum). All the specimens were thermocycled between 4°C and 60°C with 60-s dwell times for 1,000 cycles...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • Journal of biomedical optics

دوره 18 10  شماره 

صفحات  -

تاریخ انتشار 2013