Field-effect mobility of polycrystalline tetrabenzoporphyrin thin-film transistors

نویسندگان

  • Patrick B. Shea
  • Jerzy Kanicki
  • Noboru Ono
چکیده

A possible relation between a thin-film microstructure and an organic thin-film field-effect transistor OFET behavior is discussed in terms of nonlinearity in the extraction of the device electrical parameters. Staggered source and drain electrode OFETs were fabricated using a soluble precursor form of the organic small molecule semiconductor tetrabenzoporphyrin, and characterized using linear and nonlinear best-fit methods. Linear best-fit models overestimated the field-effect mobility and accumulation threshold voltage when compared to a nonlinear best-fit model that accounts for dispersive charge-carrier transport. The deviation between the methods is found to be consistently less than that for polymer OFETs, as indicated by smaller nonlinearity factors of =1.2 and 1.7 in the linear and saturation regimes, respectively. The nonlinear field-effect mobility exhibits a sublinear gate-bias dependence wherein the mobility increases at a slower rate in strong accumulation than near threshold. Furthermore, nonlinear curve fitting indicates lower trap characteristic temperatures as compared to polymer OFETs, and a relatively moderate density of grain-boundary trap states localized at the dielectric interface and in the bulk to be filled before accumulation-related conduction dominates. © 2005 American Institute of Physics. DOI: 10.1063/1.1949713

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Low Temperature Polysilicon Thin-Film Transistors on Flexible Substrates

We fabricated low-temperature polycrystalline silicon thin-film transistors (poly-Si TFTs) on flexible substrates using sputtered amorphous Si (a-Si) precursor films. The a-Si precursor films were deposited by using rf-magnetron sputtering system with argon-helium mixture gas to minimize the argon incorporation into the Si film. The a-Si films were laser annealed by using XeCl excimer laser and...

متن کامل

Effects of crystallization mechanism on the electrical characteristics of green continuous-wave-laser-crystallized polycrystalline silicon thin film transistors

Articles you may be interested in A model of electrical conduction across the grain boundaries in polycrystalline-silicon thin film transistors and metal oxide semiconductor field effect transistors Polycrystalline silicon thin-film transistors with location-controlled crystal grains fabricated by excimer laser crystallization Appl. Improvement of the electrical performance in metal-induced lat...

متن کامل

Analysis of charge transport in a polycrystalline pentacene thin film transistor by temperature and gate bias dependent mobility and conductance

The gate bias and temperature dependent field-effect mobility and conductance of a polycrystalline pentacene thin film transistor TFT were analyzed to study the charge transport in the material. Since both heating and cooling can obviously change the film morphology, a relatively narrow temperature range was adopted to rule out the possible influence of structure variation on the device charact...

متن کامل

Thin-Film Transistors in Polycrystalline Silicon by Blanket and Local Source/Drain Hydrogen Plasma-Seeded Crystallization

Thin film n-channel transistors have been fabricated in polycrystalline silicon films crystallized using hydrogen plasma seeding, by using several processing techniques with 600 to 625 C or 1000 C as the maximum process temperature. The TFT’s from hydrogen plasma-treated films with a maximum process temperature of 600 C, have a linear field-effect mobility of 35 cm/Vs and an ON/OFF current rati...

متن کامل

High electron mobility polycrystalline silicon thin-film transistors on steel foil substrates

Thin-film transistors have been fabricated in polycrystalline silicon films on steel foil. The polycrystalline silicon films were formed by the crystallization of hydrogenated amorphous silicon, which had been deposited on 200-mm-thick foils of stainless steel coated with ;0.5-mm-thick layers of SiO2. We employed crystallization temperatures ~and duration! of 600 °C ~6 h!, 650 °C ~1 h!, and 700...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2005