Natural ageing responses of duplex structured Mg-Li based alloys
نویسندگان
چکیده
Natural ageing responses of duplex structured Mg-6%Li and Mg-6%Li-6%Zn-1.2%Y alloys have been investigated. Microstructural analyses revealed that the precipitation and coarsening process of α-Mg particles could occur in β-Li phases of both two alloys during ageing process. Since a certain amount of Mg atoms in β-Li phases were consumed for the precipitation of abundant tiny MgLiZn particles, the size of α-Mg precipitates in Mg-6%Li-6%Zn-1.2%Y alloy was relatively smaller than that in Mg-6%Li alloy. Micro hardness measurements demonstrated that with the ageing time increasing, the α-Mg phases in Mg-6%Li alloy could have a constant hardness value of 41 HV, but the contained β-Li phases exhibited a slight age-softening response. Compared with the Mg-6%Li alloy, the age-softening response of β-Li phases in Mg-6%Li-6%Zn-1.2%Y alloy was much more profound. Meanwhile, a normal age-hardening response of α-Mg phases was maintained. Tensile results indicated that obvious ageing-softening phenomenon in terms of macro tensile strength occurred in both two alloys. Failure analysis demonstrated that for the Mg-6%Li alloy, cracks were preferentially initiated at α-Mg/β-Li interfaces. For the Mg-6%Li-6%Zn-1.2%Y alloy, cracks occurred at both α-Mg/β-Li interfaces and slip bands in α-Mg and β-Li phases.
منابع مشابه
The Kinetics of Natural Ageing in 6000 Alloys - a Multi-method Approach
Room temperature ‘natural’ ageing in Al-Mg-Si alloys was studied by means of six different techniques: electrical resistivity, thermoanalysis, hardness measurement, lifetime of positrons, 3D atom probe and small-angle neutron scattering in order to identify different clustering stages and to study when the negative effect of natural ageing on subsequent ‘artificial’ ageing sets in. The various ...
متن کاملTHERMAL ANALYSIS AND KINETICS OF THE PRECIPITATION IN WROUGHT Al-Mg, Al-Mg-ScAND Al-Mg-Sc-Me (Me=Zr, Ti) ALLOYS
Precipitation behaviour of wrought Al-6Mg alloys with ternary scandium and quaternary zirconium and titanium has been studied. Hardness measurements and resistivity studies are employed to assess the precipitation behaviour of scandium doped Al-6Mg alloy without or with quaternary additions of zirconium and titanium. Further, the kinetics of precipitations are studied by differential scanning c...
متن کاملMicrostructure and Precipitation in Al - Li - Cu - Mg - ( Mn , Zr ) alloys
Hot rolled Al-6Li-1Cu-1Mg-0.2Mn (at.%) (Al-1.6Li-2.2Cu-0.9Mg-0.4Mn, wt.%) and Al-6Li-1Cu-1Mg-0.03Zr (at.%) (Al-1.6Li-2.3Cu-1Mg-0.1Zr, wt.%) alloys developed for age forming were studied by tensile testing, electron backscatter diffraction (EBSD), three-dimensional atom probe (3DAP), transmission electron microscopy (TEM) and differential scanning calorimetry (DSC). For both alloys, DSC analysis...
متن کاملEffect of copper on precipitation and baking hardening behavior of Al−Mg−Si alloys
The effects of copper on the ageing precipitation behavior of as-quenched and pre-aged AA6016 aluminum alloy were studied by differential scanning calorimetry (DSC), Vickers hardness measurement and transmission electronic microscopy (TEM). The results indicate that the addition of copper facilitates the growth of clusters (GP I) to the critical size during pre-ageing. Therefore, the addition o...
متن کاملEffect of Be, Zr and Heat Treatment on Mechanical Behavior of Cast Al-Mg-Zn-Cu Alloys (7075)
The present study was undertaken to investigate the effect of aging parameters (time and temperature) on the mechanical properties of Be-and/or Zrtreated Al-Mg-Zn (7075) alloys. Ultimate tensile strength, 0.5% offset yield strength and % elongation measurements were carried out on specimens prepared from cast and heat treated 7075 alloys containing Be and/or Zr. Different aging treatment were c...