Iron-containing materials have been prepared following several strategies of synthesis and using different silica supports (amorphous, zeolitic and mesostructured materials). Activity and stability of these materials was evaluated on the wet peroxide oxidation of phenol under mild reaction conditions (100 degrees C, air pressure of 1MPa and stoichiometric amount of hydrogen peroxide for the complete mineralisation of phenol). Their catalytic performance was monitored in terms of phenol and total organic carbon (TOC) conversions, by-products distribution (aromatics compounds and carboxylic acids) and degree of metal leached into the aqueous solution. The nature and local environment of iron species is strongly dependent on the synthetic route, which dramatically influences their catalytic performance. Crystalline iron oxide species supported over mesostructured SBA-15 materials have demonstrated to be the most interesting catalysts for phenol degradation according to its high organic mineralisation, low sensitivity to leaching out and good oxidant efficiency.
منابع مشابه
Influence of textural properties and iron content on the activated carbon performance for catalytic wet air oxidation of phenol
Catalytic Wet Oxidation is a promising treatment for wastewater containing refractory compounds, such as phenol. Activated carbon has demonstrated to perform as catalyst in wet oxidation, however it is not fully understood its role as catalyst. This study aims to clarify the effect of metal content, specifically iron and calcium, on the performance of a commercial activated carbon. Several modi...
متن کاملCatalytic wet oxidation of phenol and its derivatives with Fe2O3 and MnO2
Wet oxidation of phenol, 2-chlorophenol, 4-chlorophenol and 2-nitrophenol over iron oxide and manganese dioxide catalysts was tested in this work with or without hydrogen peroxide in the reaction mixture. Influence of factors such as catalyst load, reactant-hydrogen peroxide mole ratio, and reaction time was monitored for all the phenols. Increase in the amount of hydrogen peroxide in the feed ...
متن کاملHemp Fibres as Novel Green Support Material for Immobilization of Acidithiobacillus ferrooxidans
The suitability of hemp fibres as green support material for immobilization of Acidithiobacillus ferrooxidans cells in ferrous iron bio-oxidation process was investigated. A series of experiments were carried out in shake flasks and bioreactor for both cell immobilization and iron bio-oxidation. In flask experiments, five successive batch colonization cycles resulted in 6-fold increase...
متن کاملبررسی حذف فنل از محلول های آبی با استفاده از پامیس اصلاح شده با مس
Background & Objectives: Recently, treatment of industrial wastewaters has attracted much attention of many governments and also environmental experts. Basically, these wastewaters are polluted due to the different contaminants such as dyes, halogenated hydrocarbons, phenolic compounds etc. Among these pollutants, phenols are widely used in petroleum, petrochemical, coal production and pharma...
متن کاملInfluence of Operational Parameters and Kinetic Modelling of Catalytic Wet Air Oxidation of Phenol by Al/Zr Pillared Clay Catalyst
Single and mixed oxide Al/Zr-pillared clay (Al/Zr-PILC) catalysts were synthesized and tested for catalytic wet air oxidation (CWAO) of aqueous phenol solution under milder conditions, in a semi-batch reactor. The catalysts were synthesized from natural bentonite clay using ultrasonic treatment during the aging and intercalation steps and were characterized <...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Water research
دوره 39 9 شماره
صفحات -
تاریخ انتشار 2005