The potential of triethylenetetramine (TETA) to inhibit the oxidation of pyrite in H(2)SO(4) solution had been investigated by using the open-circuit potential (OCP), cyclic voltammetry (CV), potentiodynamic polarization, and electrochemical impedance (EIS), respectively. Experimental results indicate that TETA is an efficient coating agent in preventing the oxidation of pyrite and that the inhibition efficiency is more pronounced with the increase of TETA. The data from potentiodynamic polarization show that the inhibition efficiency (η%) increases from 42.08% to 80.98% with the concentration of TETA increasing from 1% to 5%. These results are consistent with the measurement of EIS (43.09% to 82.55%). The information obtained from potentiodynamic polarization also displays that the TETA is a kind of mixed type inhibitor.
منابع مشابه
The role of catalyst in the passivation of chalcopyrite during leaching
In this work, we present as investigation of chalcopyrite leaching under different leach conditions for how liquidation and surface of chalcopyrite study using Scanning Electron Microscopy (SEM) to determine the composition of the passivation layer in the surface of chalcopyrite. The study of chalcopyrite dissolution were in H2SO4 solution systems at pH of 1.2, with 5% chalcopyrite concentrate ...
متن کاملAn investigation on the passivation behavior of nitrogen enriched AISI 316L austenitic stainless steel
In the present work the effects of plasma nitridization on the passivation behavior of AISI 316L was investigated. To do this; nitriding treatments were carried out at 420°C for 1, 2, 4 and 16 hours. The phase composition and structure of the nitrided layer were studied by Low Angle X-ray diffraction and Scanning Electron Microscopy. The hardness of samples also was evaluated by Vickers microha...
متن کاملControl of Acid Generation from Pyrite Oxidation in a Highly Reactive Natural Waste: A Laboratory Case Study
Laboratory kinetic leach column (KLC) tests were carried out to define the conditions required to control acid generation from a highly reactive, potentially acid-forming (PAF) iron ore waste rock. It was found that lime addition (0.1 wt % blended) plus either blending of silicates (25 wt % K-feldspar and 25 wt % chlorite), or addition of a non-acid forming (NAF) top cover containing about 10% ...
متن کاملGrowth Defects and Chromium Content Loss during the Deposition of Stainless Steel by CAE-PVD and Its Effect on the Corrosion and Passivation Behavior of the Coating
In the present study, the effects of growth defects and chromium content loss on the degradation of corrosion and passivation of cathodic arc evaporation (CAE-PVD) of stainless steel coating were investigated in 2 M sulphuric acid solution. EDS analysis indicated that the micro-particles were obtained during the coating growth. In addition, it was detected that the growth defects had poor adhes...
متن کاملCorrosion and Electrochemical Oxidation of a Pyrite by Thiobacillus ferrooxidans.
The oxidation of a pure pyrite by Thiobacillus ferrooxidans is not really a constant phenomenon; it must be considered to be more like a succession of different steps which need characterization. Electrochemical studies using a combination of a platinum electrode and a specific pyrite electrode (packed-ground-pyrite electrode) revealed four steps in the bioleaching process. Each step can be ide...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
دوره 2013 شماره
صفحات -
تاریخ انتشار 2013