Morphologies and kinetics of a dewetting ultrathin solid film

نویسندگان

  • Mikhail Khenner
  • M. Khenner
چکیده

Abstract The surface evolution model based on geometric partial differential equation is used to numerically study the kinetics of dewetting and dynamic morphologies for the localized pinhole defect in the surface of the ultrathin solid film with the strongly anisotropic surface energy. Depending on parameters such as the initial depth and width of the pinole, the strength of the attractive substrate potential and the strength of the surface energy anisotropy, the pinhole may either extend to the substrate and thus rupture the film, or evolve to the quasiequilibrium shape while the rest of the film surface undergoes phase separation into a hill-and-valley structure followed by coarsening. Overhanging (non-graph) morphologies are possible for deep, narrow (slit-like) pinholes.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Structure Formation of Ultrathin PEO Films at Solid Interfaces—Complex Pattern Formation by Dewetting and Crystallization

The direct contact of ultrathin polymer films with a solid substrate may result in thin film rupture caused by dewetting. With crystallisable polymers such as polyethyleneoxide (PEO), molecular self-assembly into partial ordered lamella structures is studied as an additional source of pattern formation. Morphological features in ultrathin PEO films (thickness < 10 nm) result from an interplay b...

متن کامل

Mikhail Khenner Department of Mathematics State University of New York at Buffalo

2.1 Stability of fluid surfaces and interfaces in the vibration fields: pp. 3 4 2.2 Grain-boundary grooving by surface diffusion and electromigration: pp. 4 5 2.3 Selective Area Epitaxy (SAE) and Electroepitaxy (SAEE): pp. 5 6 2.4 Directed self-assembly in the nonuniform temperature fields: p. 7 2.5 Dynamics and morphologies of a dewetting ultrathin solid films: p. 8 2.6 Stability of deposited ...

متن کامل

Dewetting of thin polymer films near the glass transition.

Dewetting of ultrathin polymer films near the glass transition exhibits unexpected front morphologies [G. Reiter, Phys. Rev. Lett. 87, 186101 (2001)]. Here, we present the first theoretical attempt to understand these features, focusing on the shear-thinning behavior of these films. We analyze the profile of the dewetting film, and characterize the time evolution of the dry region radius, R(d)(...

متن کامل

AFM analysis of high temperature dewetting under ultra high vacuum of ultrathin solid silicon films on insulator

The dewetting of ultrathin silicon layers, induced by the thermal budget, is an issue to develop SOI-based technology. This study aims at demonstrating the effect of the strain on the dewetting mechanism [1] (Figure 1). For that purpose, we present the results obtained on (001) oriented ultrathin (<11 nm) silicon layers on silicon dioxide (SOI). Both stress-free and strained (s-SOI) films fabri...

متن کامل

Comparative study of a solid film dewetting in an attractive substrate potentials with the exponential and the algebraic decay

Abstract We compare dewetting characteristics of a thin nonwetting solid film in the absence of stress, for two models of a wetting potential: the exponential and the algebraic. The exponential model is a one-parameter (r) model, and the algebraic model is a two-parameter (r, m) model, where r is the ratio of the characteristic wetting length to the height of the unperturbed film, and m is the ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2013