Combined Kinetic Analysis of Thermal Degradation of Polymeric Materials under Any Thermal Pathway
نویسندگان
چکیده
Combined kinetic analysis has been applied for the first time to the thermal degradation of polymeric materials. The combined kinetic analysis allows the determination of the kinetic parameter from the simultaneous analysis of a set of experimental curves recorded under any thermal schedule. Besides, the method does not make any assumption about the kinetic model or activation energy and allows the analysis even when the process does not follow one of the ideal kinetic models already proposed in literature. In the present paper the kinetics of the thermal degradation of both polytetrafluoroethylene (PTFE) and polyethylene (PE) have been performed. It has been concluded, without previous assumptions on the kinetic model, that the thermal degradation of PTFE obeys a first order kinetic law, while the thermal degradation of PE follows a diffusion-controlled kinetic model.
منابع مشابه
Rapid Synthesis of Nanostructured Pure Anatase TiO2 with High Thermal Stability by Polymeric Sol-Gel Route
The nanostructured anatase TiO2 with high thermal stability was prepared by polymeric sol-gel method without any additives. The particle size distribution of polymeric titania sol was determined by dynamic light scattering (DLS). Then properties of obtained titania were investigated by TG-DTA, XRD, FESEM and TEM. Also, the decolorization capability of resultant anatase was evaluated using methy...
متن کاملThermal Degradation Kinetic Study of a Fuel-rich Energetic Mixture Containing Epoxy Binder
In this work, thermal degradation behavior of a fuel-rich energetic mixture containing epoxy binder was studied by thrmogravimetric analysis and differential scanning calorimetry under dynamic nitrogen atmosphere at different heating rates. Variation of the thermal degradation activation energy of the mixture was evaluated by differential and integral isoconversional methods via ...
متن کاملThermal and catalytic degradation study of polyethylene and investigation the catalytic effect of X-Zeolite and Silica-Alumina on degradation kinetic
The thermal degradation of polyethylene (PE) was carried out in the absence and presence ofcatalystes X-Zeolite and Silica-Alumina at different temperatures. The optimum PE/Catalysisratio was 0.25:0.05 g/g, which produced highest degradation value. PE and PE/Catalysis werecharacterized by thermogravimetric analysis. The thermal degradation properties of polymerhave been studied by Infrared spec...
متن کاملSurface Degradation of Polymer Matrix Composites Under Different Low Thermal Cycling Conditions
The principal effects of mass degradation on polymer matrix composites (PMCs) are the decay of mechanical properties such as strength, elongation, and resilience. This degradation is a common problem of the PMCs under thermal cycling conditions. In this article, composite degradation was investigated by measurement of total mass loss (TML) using the Taguchi approach. Thermal cycling tests were ...
متن کاملThe Kinetic and Thermal Degradation Studies of N-(4-Acetyl-phenyl)-acetimidic Acid Pyridine-3-yl ester Metal(II) Complexes
Schiff base complexes of transition metals are of particular interest to inorganic chemists because of their structural, spectral and chemical properties, which are often strongly dependant on the nature of the ligand structure. Large number of metal (II) complexes with Schiff-base ligands has been extensively studied for their interesting structural specialties, applications and properties. Th...
متن کامل