Porcelain surface-conditioning techniques and the shear bond strength of ceramic brackets.
نویسندگان
چکیده
The aim of this study was to compare the effects of various porcelain surface-conditioning techniques, used either alone or in combination, on the shear bond strength (SBS) of ceramic brackets cured with a light emitting diode (LED). Thirty glazed porcelain facets were randomly divided into three groups of 10. In group I, the porcelain surfaces were etched with 9.6 per cent hydrofluoric acid (HFA) for 2 minutes before silane application, in group II, the porcelain surfaces were sandblasted with aluminium oxide particles, etched with 9.6 per cent HFA for 2 minutes, and silane applied, and in group III, the porcelain surfaces were sandblasted with aluminium oxide particles before silane application. Spirit ceramic brackets were bonded with a light-cured composite resin (Light Bond) and a LED. All specimens were stored in distilled water at 37 degrees C for 24 hours and thermocycled. Bond strength was determined in shear mode at a crosshead speed of 0.5 mm/minute until fracture occurred. Analysis of variance indicated a significant difference between groups (P < 0.001). The lowest SBS was found in group III (5.46 +/- 1.34, P < 0.001). No significant difference was found between group I (11.38 +/- 1.65) and group II (10.45 +/- 1.15; P > 0.05). Surface treatment with HFA and a silane coupling agent produced the highest bond strength. Sandblasting before HFA and silane application did not significantly increase bond strength. Silane application to sandblasted porcelain provided poor results in vitro and clinical trials are needed to determine its reliability for bonding ceramic brackets to ceramic crowns.
منابع مشابه
Comparison of shear bond strength of metal brackets bonded to porcelain surface using different surface conditioning methods: an in vitro study.
AIM To evaluate and compare the shear bond strength of metal brackets bonded to ceramic surfaces using different conditioning methods and to assess the site of bond failure after debonding. MATERIALS AND METHODS A total of 70 ceramic surfaces were produced with uniform shape, size and composition. The samples were divided into 7 groups (each of 10 samples). Group 1 was the control group (untr...
متن کاملFour chemical methods of porcelain conditioning and their influence over bond strength and surface integrity.
OBJECTIVE To assess four different chemical surface conditioning methods for ceramic material before bracket bonding, and their impact on shear bond strength and surface integrity at debonding. METHODS Four experimental groups (n = 13) were set up according to the ceramic conditioning method: G1 = 37% phosphoric acid etching followed by silane application; G2 = 37% liquid phosphoric acid etch...
متن کاملThe Effect of Remin Pro and MI Paste Plus on Bleached Enamel Surface Roughness
OBJECTIVE Increased number of adult patients requesting orthodontic treatment result in bonding bracket to ceramic restorations more than before. The aim of this study was to evaluate and compare the shear bond strength of orthodontic brackets bonded to two types of ceramic bases with conventional orthodontic bonding resin and a new nano-filled composite resin. MATERIALS AND METHODS Twenty fo...
متن کاملShear Bond Strength of Metallic and Ceramic Brackets Bonded with Two-step and Three-step Light Cure Adhesives
Background and purpose: The bonding process is highly important in orthodontic treatment for its fast speed. The purpose of this study was to compare the shear bond strength of ceramic and metallic brackets between three stage (transbondTM XT) and two stage (GC ortho connectTM) light cure composites. Materials and methods: In this experimental study, 80 maxillary and mandibular first and sec...
متن کاملEffect of Silane on Shear Bond Strength of Two Porcelain Repair Systems
Objectives: Ceramics have advantages such as optimal esthetics and biocompatibility. However, in the oral environment, they are subjected to high levels of stress due to masticatory forces, saliva, thermal changes and alterations of pH, which increase their risk of fracture. Since replacement of these restorations is costly and time-consuming, composite resin is often used for intraoral repair ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- European journal of orthodontics
دوره 28 5 شماره
صفحات -
تاریخ انتشار 2006