Background The aim of this in vitro study was to evaluate the color stability of CAD/CAM Zirconia ceramics following exposure to acidic drink (Coca Cola) and after exposure to staining solution (coffee). Material and Methods All the samples were immersed in different staining solutions over a 28-day test period. A colorimetric evaluation according to the CIE L*a*b* system was performed by a blind trained operator at 7, 14, 21, 28 days of the staining process. Shapiro Wilk test and Kruskal-Wallis ANOVA were applied to assess significant differences among restorative materials. Paired t-test was applied to test which CIE L*a*b* parameters significantly changed after immersion in staining solutions. Results One week immersion in acidic drink did not cause a perceivable discoloration for all restorative materials (ΔE < 3.3). Subsequent immersion in coffee affected color stability of all Zirconia samples, even if Kruskal-Wallis ANOVA found significant differences among the various restorative materials. Conclusions The ∆Es of CAD/CAM Zirconia ceramics after immersion in coffee varied among the products, but color integrity is not affected by contact with acidic drinks. Key words:CAD/CAM restorative materials, CIE Lab, Zirconia ceramics.
منابع مشابه
The effect of different surface treatment methods on the color stability of monolithic zirconia
Abstract Background & aim: There are so many studies about effect of colored drinks and mouthwashes on discoloration of different dental ceramics. However, little is known regarding the effect of colored drinks on discoloration of monolithic zirconia .The purpose of this invitro study was to evaluate the effect of different surface treament methods on color stability of monolithic zirconia....
متن کاملThe Effect of Different Solutions on Optical Behavior of Polished and Glazed Zirconia-Reinforced Lithium Silicate Ceramics
Background: This study sought to assess the effect of glazing and polishing surface treatments on the optical behavior of zirconia-reinforced lithium silicate ceramics thermocycled in different solutions. Methods:Computer-aided design/computer-aided manufacturing ceramics (VITA Suprinity) were cut into samples (n=104) measuring 1.5x14x10 mm according to t...
متن کاملLess Light Transmitted Through Zirconia Copings Translucency of Zirconia Copings Made With Different
Background: There is increased use of all-ceramic crowns in place of ceramo-metal crowns in restorative practices. The difference in properties of different ceramics will affect the final esthetics of the restoration, and we need to consider this, especially when restoring anterior teeth. This article compares and analyzes translucency levels of different zirconia-based ceramic CAD/CAM systems....
متن کاملThe Effect of Different Finishing Lines on the Marginal Fitness of Full Contour Zirconia and Glass Ceramic CAD/CAM Crowns (An in-vitro study)
Purpose: The aim of this study was to evaluate the effect of two gingival finishing lines (90° shoulder and deep chamfer) on the marginal fitness of two types of full anatomic all-ceramic crowns; zirconia crowns (Zikonzhan) and glass ceramic crowns (IPS e-max CAD) milled with CAD/CAM system. Materials and Methods: Two dentoform teeth of left maxillary first molar were prepared with chamfer fini...
متن کاملCurrent status of zirconia restoration.
During the past decade, zirconia-based ceramics have been successfully introduced into the clinic to fabricate fixed dental prostheses (FDPs), along with a dental computer-aided/computer-aided manufacturing (CAD/CAM) system. In this article (1) development of dental ceramics, (2) the current status of dental CAD/CAM systems, (3) CAD/CAM and zirconia restoration, (4) bond between zirconia and ve...
متن کامل