This study evaluated the bond strength of brackets to ceramic testing different etching times and light sources for photo-activation of the bonding agent. Cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 20 or 60 s. After application of silane on the ceramic surface, metallic brackets were bonded to the cylinders using Transbond XT (3M Unitek). The specimens for each etching time were assigned to 4 groups (n=15), according to the light source: XL2500 halogen light, UltraLume 5 LED, AccuCure 3000 argon laser, and Apollo 95E plasma arc. Light-activation was carried out with total exposure times of 40, 40, 20 and 12 s, respectively. Shear strength testing was carried out after 24 h. The adhesive remnant index (ARI) was evaluated under magnification. Data were subjected to two-way ANOVA and Tukey's test (α=0.05). Specimens etched for 20 s presented significantly lower bond strength (p<0.05) compared with those etched for 60 s. No significant differences (p>0.05) were detected among the light sources. The ARI showed a predominance of scores 0 in all groups, with an increase in scores 1, 2 and 3 for the 60 s time. In conclusion, only the etching time had significant influence on the bond strength of brackets to ceramic.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Saliva Contamination and sequencing time of curing the Transbond™ Plus Self Etching Primer on the Shear Bond Strength of Orthodontic Brackets

Abstract Background and aim: Over the years, improvments have been done to simplify clinical bonding procedure. One of these material is Transbond™ Plus Self Etching. The aim of this study was to evaluate the effect of saliva contamination and reusing Transbond™ Plus Self Etching Primer (SEP) on shear bond strength of orthodontic brackets. Materials and Methods: Fifty premolars divided into fiv...

متن کامل

Shear Bond Strength of Metallic and Ceramic Brackets Bonded with Two-step and Three-step Light Cure Adhesives

  Background and purpose: The bonding process is highly important in orthodontic treatment for its fast speed. The purpose of this study was to compare the shear bond strength of ceramic and metallic brackets between three stage (transbondTM XT) and two stage (GC ortho connectTM) light cure composites. Materials and methods: In this experimental study, 80 maxillary and mandibular first and sec...

متن کامل

Effect of bonding material, etching time and silane on the bond strength of metallic orthodontic brackets to ceramic.

The purpose of this study was to evaluate the bond strength of metallic orthodontic brackets to feldspathic ceramic with different etching times, bonding materials and with or without silane application. Cylinders of feldspathic ceramic were etched with 10% hydrofluoric acid for 20 or 60 s. For each etching time, half of the cylinders received two layers of silane. Metallic brackets were bonded...

متن کامل

Comparison of shear bond strength of the stainless steel metallic brackets bonded by three bonding systems

Introduction: In orthodontic treatment, it is essential to establish a satisfactory bond between enamel and bracket. After the self-etch primers (SEPs) were introduced for the facilitation of bracket bonding in comparison to the conventional etch-and-bond system, multiple studies have been carried out on their shear bond strengths which have yielded different results. This study was aimed at co...

متن کامل

Effect of hydrofluoric acid concentration and etching time on microtensile bond strength of suprinity and enamic CAD/CAM ceramics to resin cement

Introduction: The use of dental ceramics has increased due to their beauty and biocompatibility. The aim of this study was to evaluate the effect of hydrofluoric acid concentration and etching time on microtensile bond strength (μTBS) of the Enamic and Suprinity ceramics. Material & Methods: In this in vitro study, two hydrofluoric acid (HFA) concentrations of 5% (A) and 10% (B) were used at t...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

عنوان ژورنال:
  • Brazilian dental journal

دوره 22 3  شماره 

صفحات  -

تاریخ انتشار 2011