Initial stages of oxide formation on the Zr surface at low oxygen pressure: An in situ FIM and XPS study
نویسندگان
چکیده
An improved methodology of the Zr specimen preparation was developed which allows fabrication of stable Zr nanotips suitable for FIM and AP applications. Initial oxidation of the Zr surface was studied on a Zr nanotip by FIM and on a polycrystalline Zr foil by XPS, both at low oxygen pressure (10(-8)-10(-7)mbar). The XPS data reveal that in a first, fast stage of oxidation, a Zr suboxide interlayer is formed which contains three suboxide components (Zr(+1), Zr(+2) and Zr(+3)) and is located between the Zr surface and a stoichiometric ZrO2 overlayer that grows in a second, slow oxidation stage. The sole suboxide layer has been observed for the first time at very early states of the oxidation (oxygen exposure ≤ 4L). The Ne(+) FIM observations are in accord with a two stage process of Zr oxide formation.
منابع مشابه
THE ACTIVATION OF CARBON DIOXIDE AT A MAGNESIUM (1 00) SURFACE THE ROLE OF OXYGEN TRANSIENTS
X-ray photoelectron and high resolution electron energy loss spectroscopic (XPS-HREELS) studies have shown that the adsorption of carbon dioxide at Mg(100) surfaces at 80K is followed by a dissociative reaction leading to the formation of a metastable surface carbonate above 80K. The formation of a carbonate species is proposed to proceed through oxidation of C0 (g) by an active oxygen su...
متن کاملCoadsorption of Dioxygen and Carbon Monoxide on a Mg(100) Surface
The activation of carbon monoxide by oxygen on Mg(100) surface has been investigated by X-ray photoelectron spectroscopy (XPS). Carbon monoxide is only weakly adsorbed (dispersion-type forces) on a magnesium surface. The XPS result has shown that the dissociation of carbon monoxide leading to the formation of a metastable surface carbonate species occurs through the participation of an oxyg...
متن کاملInfluence of Operational Parameters and Kinetic Modelling of Catalytic Wet Air Oxidation of Phenol by Al/Zr Pillared Clay Catalyst
Single and mixed oxide Al/Zr-pillared clay (Al/Zr-PILC) catalysts were synthesized and tested for catalytic wet air oxidation (CWAO) of aqueous phenol solution under milder conditions, in a semi-batch reactor. The catalysts were synthesized from natural bentonite clay using ultrasonic treatment during the aging and intercalation steps and were characterized <...
متن کاملPhotoemission measurements of Ultrathin SiO2 film at low take-off angles
The surface and interfacial analysis of silicon oxide film on silicon substrate is particularly crucial in the nano-electronic devices. For this purpose, series of experiments have been demonstrated to grow oxide film on Si (111) substrate. Then these films have been used to study the structure of the film by using X-ray photo emission spectroscopy (XPS) technique. The obtained results indicate...
متن کاملSilicon Oxide Surface Segregation in CO Oxidation on Pd: An in situ PEEM, MS and XPS Study
ABSTRACT The effect of silicon oxide surface segregation on the locally-resolved kinetics of the CO oxidation reaction on individual grains of a polycrystalline Pd foil was studied in situ by PEEM, MS and XPS. The silicon oxide formation induced by Si-impurity segregation at oxidizing conditions, was monitored by XPS and its impact on the global and local (spatially resolved) kinetics of the CO...