Early complications and performance of 327 heat-pressed lithium disilicate crowns up to five years

نویسندگان

  • Fabian Huettig
  • Ulf Peter Gehrke
چکیده

PURPOSE The prospective follow-up aimed to assess the performance of lithium disilicate crowns and clinical reasons of adverse events compromising survival and quality. MATERIALS AND METHODS 58 patients were treated with 375 heat-pressed monolithic crowns, which were bonded with resin cement. Annual recalls up to five years included a complete dental examination as well as quality assessment using CDA-criteria. Any need for clinical intervention led to higher complication rate and any failure compromised the survival rate. Kaplan-Meier-method was applied to all crowns and a dataset containing one randomly selected crown from each patient. RESULTS Due to drop-outs, 45 patients (31 females, 14 males) with the average age of 43 years (range = 17-73) who had 327 crowns (176 anterior, 151 posterior; 203 upper jaw, 124 lower jaw) were observed and evaluated for between 4 and 51 months (median = 28). Observation revealed 4 chippings, 3 losses of retention, 3 fractures, 3 secondary caries, 1 endodontic problem, and 1 tooth fracture. Four crowns had to be removed. Survival and complication rate was estimated 98.2% and 5.4% at 24 months, and 96.8% and 7.1% at 48 months. The complication rate was significantly higher for root canal treated teeth (12%, P<.01) at 24 months. At the last observation, over 90% of all crowns showed excellent ratings (CDA-rating Alfa) for color, marginal fit, and caries. CONCLUSION Heat pressed lithium disilicate crowns showed an excellent performance. Besides a careful luting, dentists should be aware of patients' biological prerequisites (grade of caries, oral hygiene) to reach full success with these crowns.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Lithium Disilicate Reinforced Liner Treatment on Bond and Fracture Strengths of Bilayered Zirconia All-Ceramic Crown

This study was performed to evaluate the effect of a lithium-disilicate spray-liner application on both the bond strength between zirconia cores and heat-pressed lithium-disilicate glass-ceramic veneers, and the fracture strength of all-ceramic zirconia crowns. A lithium-disilicate reinforced liner was applied on the surface of a zirconia core and lithium-disilicate glass-ceramic was veneered o...

متن کامل

Multifunctional uses of a novel ceramic-lithium disilicate.

Objective: To familiarize the reader with the material characteristics of and indications for lithium disilicate ceramic. Summary: This paper is part of the Journal's "Masters of Esthetic Dentistry" feature. Lithium disilicate is a glass ceramic material that can be used to form restorations using either a lost-wax hot pressing technique or CAD/CAM milling procedures. Although the pressable and...

متن کامل

Porcelain-Fused-to-Metal and All-Ceramic Crowns for Posterior Teeth: Material science and Laboratory Procedures

QDT 2013 Over the last decade, laboratory procedures have changed dramatically due to the introduction of computer-aided design/computerassisted manufacture (CAD/CAM) technology. This evo lu tion began with the use of zirconia as a base material for dental restorations. Recently, the use of CAD/CAM-fabricated full-contour zirconia (FCZ) crowns for posterior teeth has become a popular restoratio...

متن کامل

Bonding lithium disilicate ceramic to feather-edge tooth preparations: a minimally invasive treatment concept.

PURPOSE To report the short-term clinical outcome of a new minimally invasive prosthetic approach utilizing monolithic lithium-disilicate full crowns bonded to feather-edge tooth preparations. MATERIALS AND METHODS 235 teeth, 136 anterior and 99 posterior, requiring a full crown were prepared with a feather-edge finish line providing a minimum space on the vertical walls of 0.3 mm at the marg...

متن کامل

Effect of Different Luting Agents on the Retention of Lithium Disilicate Ceramic Crowns

No studies are available that evaluate the retention of disilicate crowns according to different cementation procedures. The purpose of this study was to measure the retention of lithium disilicate crowns cemented using two different cementation systems. Twenty extracted mandibular premolars were prepared. Anatomic crowns were waxed and hot pressed using lithium disilicate ceramic. Teeth were d...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 8  شماره 

صفحات  -

تاریخ انتشار 2016