Improvement of the Cathode Electrolyte Interphase on P2-Na2/3Ni1/3Mn2/3O2 by Atomic Layer Deposition.

نویسندگان

  • Judith Alvarado
  • Chuze Ma
  • Shen Wang
  • Kimberly Nguyen
  • Moses Kodur
  • Ying Shirley Meng
چکیده

Atomic layer deposition (ALD) is a commonly used coating technique for lithium ion battery electrodes. Recently, it has been applied to sodium ion battery anode materials. ALD is known to improve the cycling performance, Coulombic efficiency of batteries, and maintain electrode integrity. Here, the electrochemical performance of uncoated P2-Na2/3Ni1/3Mn2/3O2 electrodes is compared to that of ALD-coated Al2O3 P2-Na2/3Ni1/3Mn2/3O2 electrodes. Given that ALD coatings are in the early stage of development for NIB cathode materials, little is known about how ALD coatings, in particular aluminum oxide (Al2O3), affect the electrode-electrolyte interface. Therefore, full characterizations of its effects are presented in this work. For the first time, X-ray photoelectron spectroscopy (XPS) is used to elucidate the cathode electrolyte interphase (CEI) on ALD-coated electrodes. It contains less carbonate species and more inorganic species, which allows for fast Na kinetics, resulting in significant increase in Coulombic efficiency and decrease in cathode impedance. The effectiveness of Al2O3 ALD coating is also surprisingly reflected in the enhanced mechanical stability of the particle which prevents particle exfoliation.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Electrochemical and thermal properties of P2-type Na2/3Fe1/3Mn2/3O2 for Na-ion batteries

P2-type Na2/3Fe1/3Mn2/3O2 was prepared by means of solid-state reaction. Its electrochemical properties as a cathode for sodium-ion batteries were investigated in the 1.5e4.3 V range vs. Na metal. This material delivers an initial discharge capacity as high as 193 mAh/g and maintains 153 mAh/g in 40 cycles. Such a high reversible capacity is achieved because both Mn3þ/Mn4þ and Fe3þ/Fe4þ become ...

متن کامل

Direct evidence for high Na+ mobility and high voltage structural processes in P2-Nax[LiyNizMn1−y−z]O2 (x, y, z ≤ 1) cathodes from solid-state NMR and DFT calculations

Department of Chemistry, University of E-mail: [email protected] Department of NanoEngineering, Universit 92037, USA Department of Materials Science and Engi 50011, USA Department of Chemistry, University of Wa † Electronic supplementary information data for P2-Na2/3Ni1/3Mn2/3O2; ts o electrochemically-cycled P2-NaxNi1/3Mn2/ XRD data for a 4.4 V charged P2-NaxL computational details for the CRYS...

متن کامل

Na+/vacancy disordering promises high-rate Na-ion batteries

As one of the most fascinating cathode candidates for Na-ion batteries (NIBs), P2-type Na layered oxides usually exhibit various single-phase domains accompanied by different Na+/vacancy-ordered superstructures, depending on the Na concentration when explored in a limited electrochemical window. Therefore, their Na+ kinetics and cycling stability at high rates are subjected to these superstruct...

متن کامل

Facile synthesis of hierarchical fern leaf-like Sb and its application as an additive-free anode for fast reversible Na-ion storage

Hierarchical Sb was successfully fabricated via a very simple and cost-effective electrochemical deposition method. Morphological and structural characterizations show that the as-prepared Sb has a uniform fern leaf-like structure which is composed of well-crystallized Sb nanoparticles. The formation mechanism of the fern leaf-like Sb was also investigated. The hierarchical Sb exhibits desirabl...

متن کامل

Comparison between ultrathin films of YSZ deposited at the solid oxide fuel cell cathode/electrolyte interface by atomic layer deposition, dip-coating or sputtering

The effect of an 80 nm YSZ interfacial layer, deposited onto a YSZ pellet by different techniques (dip-coating, sputtering and atomic layer deposition) at the SOFC cathode/electrolyte interface to allow a maximum adhesion of the thick cathode layer, was thoroughly analysed. The LSM cathode was deposited on the solid electrolyte by painting and sintered in air at 1200°C for 2 h. The morphologica...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:
  • ACS applied materials & interfaces

دوره 9 31  شماره 

صفحات  -