This study evaluated the impact of extended etching and bonding strategies on the microshear bond strength of three sealant materials. Two pit-and-fissure sealants [FluroShield, Dentsply (light-cured) and AlphaSeal, DFL (self-cured)] and one light-cured flowable composite resin (Permaflo, Ultradent) were evaluated according to different enamel etching times (15 s or 30 s) and bonding procedures (no adhesive application, application of primer/hydrophobic resin or hydrophobic resin only). Intact enamel blocks were obtained from bovine teeth and sealed via the tested protocols. After 24 h, the microshear bond strength test was performed in a universal testing machine at a crosshead speed of 0.5 mm/min. Failure modes were classified by stereomicroscopy. Data were submitted to a three-way ANOVA and to Tukey's test (α=0.05). There was no statistically significant difference (p>0.05) among the materials. Permaflo showed higher bond strength when etched for 30 s alone. Enamel overetching decreased the bond strength of the light-cured sealant. Primer/bond previous treatment improved bond performance for AlphaSeal. In conclusion, from the tested conditions, all sealant materials presented similar bond strength values in relation to bonding protocol and etching time. The flowable composite can be used as a pit-and-fissure sealant. The use of a three-step adhesive system was essential for the self-cured sealant application.
منابع مشابه
Assessment of Microshear Bond Strength: Self-Etching Sealant versus Conventional Sealant
OBJECTIVE Recently, self-etching fissure sealants have been introduced to reduce technical sensitivity; however, their efficacy should be assessed. The aim of this study was to assess of the microshear bond strength of self-etching and conventional fissure sealants. MATERIALS AND METHODS Thirty non-carious third molars were randomly divided into three groups (N=10). Microcylinders of Concise ...
متن کاملEffect of chlorhexidine solution on microleakage of pit and fissure sealants in permanent teeth with and without the use of fifth- and sixth-generation adhesive systems
Introduction: Due to concerns about histological caries and recurrent caries after the use of sealants, adhesive systems containing fluoride and antibacterial agents have been proposed. The aim of this study was to evaluate the microleakage of sealants after the use of antibacterial chlorhexidine solution on etched enamel with and without the use of fifth- and sixth-generation adhesive systems....
متن کاملEffect of 20- or 60-second curing times on retention of five sealant materials.
F or adequate sealant retention, the bonding surface area must be maximized and the enamel clean, free of salivary contamination, and dry at the time of sealant placement.I, 2 However, because pit and fissure sealants bond to the cuspal incline planes and not to the bottoms of the pits and fissures,B_6 insufficient curing of the resin sealant could reduce the bond strength. The purpose of this ...
متن کاملAn evaluation on the effects of 37% phosphoric acid and self – etching primer on shear bond strength of enamel
An evaluation on the effects of 37% phosphoric acid and self – etching primer on shear bond strength of enamel Dr. A. Davari* - Dr. H. Hajizadeh* - Dr. H. Sharifikhatoonabadi** *- Assistant Professor of Operative Dentistry Dept. - Faculty of Dentistry - Yazd University of Medical Sciences. **- Dentist. Background and Aim: The goal of this study was to evaluate the effects of 37% phosphoric acid...
متن کاملEffect of Saliva Contamination and sequencing time of curing the Transbond™ Plus Self Etching Primer on the Shear Bond Strength of Orthodontic Brackets
Abstract Background and aim: Over the years, improvments have been done to simplify clinical bonding procedure. One of these material is Transbond™ Plus Self Etching. The aim of this study was to evaluate the effect of saliva contamination and reusing Transbond™ Plus Self Etching Primer (SEP) on shear bond strength of orthodontic brackets. Materials and Methods: Fifty premolars divided into fiv...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Brazilian dental journal
دوره 23 5 شماره
صفحات -
تاریخ انتشار 2012