Effect of hydration variability on hybrid layer properties of a self-etching versus an acid-etching system.
نویسندگان
چکیده
The hypothesis tested in this study was that the self-etching system (Clearfil SE Bond, CSE) is less sensitive to surface moisture variability than the system that uses a separate acid-etching step (Single Bond, SB). Eighteen dentin specimens were bonded to composite using CSE or SB. Three different surface moisture conditions per bonding type (overwet, w; dry, d; and visibly moist, n [normal]) were applied prior to bonding dentin to composite. One cross section of each sample was analyzed with lines of nanoindentations crossing perpendicular to the bonding interface. An additional set of bonded samples was fixed and cross sectioned before the hybrid layer thickness was measured in scanning electron microscopy. The nanoindentations revealed significant differences in indentation modulus (E(i)) and hardness (H) for the hybrid layer comparing SBn, E(i) = 2.7(+/-1.6); H = 0.24(+/-0.1) GPa with SBd, E(i) = 0.9(+/-0.7); H = 0.9(+/-0.05) GPa, respectively, while CSE showed no differences among the groups. A significantly greater demineralized zone below the hybrid layer was found for SBd. The hybrid layer was wider for both CSEd and SBd. In conclusion the hypothesis was verified; CSE exhibited no significant changes of hybrid layer properties (E(i), H) at different hydration conditions, while SB had significant differences, especially after air-drying.
منابع مشابه
An evaluation on the effects of 37% phosphoric acid and self – etching primer on shear bond strength of enamel
An evaluation on the effects of 37% phosphoric acid and self – etching primer on shear bond strength of enamel Dr. A. Davari* - Dr. H. Hajizadeh* - Dr. H. Sharifikhatoonabadi** *- Assistant Professor of Operative Dentistry Dept. - Faculty of Dentistry - Yazd University of Medical Sciences. **- Dentist. Background and Aim: The goal of this study was to evaluate the effects of 37% phosphoric acid...
متن کاملInvestigation of HF/H2O2 Concentration Effect on Structural and Antireflection Properties of Porous Silicon Prepared by Metal-Assisted Chemical Etching Process for Photovoltaic Applications
Porous silicon was successfully prepared using metal-assisted chemical etching method. The Effect of HF/H2O2 concentration in etching solution as an affecting parameter on the prepared porosity type and size was investigated. Field emission electron microscopy (FE-SEM) confirmed that all etched samples had porous structure and the sample which was immersed into HF/H2O2 withmolar ratio of 7/3.53...
متن کاملEffect of Saliva Contamination and sequencing time of curing the Transbond™ Plus Self Etching Primer on the Shear Bond Strength of Orthodontic Brackets
Abstract Background and aim: Over the years, improvments have been done to simplify clinical bonding procedure. One of these material is Transbond™ Plus Self Etching. The aim of this study was to evaluate the effect of saliva contamination and reusing Transbond™ Plus Self Etching Primer (SEP) on shear bond strength of orthodontic brackets. Materials and Methods: Fifty premolars divided into fiv...
متن کاملEffect of hydrofluoric acid concentration and etching time on the surface roughness of CAD/CAM ceramics
Introduction: Dental ceramics are considered as materials that can restore the appearance of natural teeth. Etching the inner surface of a ceramic restoration with hydrofluoric acid (HF) followed by using a silane coupling agent is a well-known and recommended method to increase the bond strength. The aim of etching on ceramic structure is to enhance the surface roughness (Ra) and energy and to...
متن کاملStructural and optical properties of n- type porous silicon– effect of etching time
Porous silicon layers have been prepared from n-type silicon wafers of (100) orientation. SEM, FTIR and PL have been used to characterize the morphological and optical properties of porous silicon. The influence of varying etching time in the anodizing solution, on structural and optical properties of porous silicon has been investigated. It is observed that pore size increases with etching tim...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Biomaterials
دوره 26 9 شماره
صفحات -
تاریخ انتشار 2005