Effect of microwave annealing temperatures on lead zirconate titanate thin films.
نویسندگان
چکیده
Lead zirconate titanate (Pb(1.1)(Zr(0.52)Ti(0.48))O(3)) thin films of thickness 260 nm on Pt/Ti/SiO(2)/Si substrates were densified by 2.45 GHz microwave annealing. The PZT thin films were annealed at various annealing temperatures from 400 to 700 °C for 30 min. X-ray diffraction showed that the pyrochlore phase was transformed to the perovskite phase at 450 °C and the film was fully crystallized. The secondary (again pyrochlore) phase was observed in the PZT thin films, which were annealed above 550 °C. The surface morphologies were changed above 550 °C of the PZT thin films due to the secondary phase. Higher dielectric constant (ε(r)) and lower dielectric loss coercive field (E(c)) were achieved for the 450 °C film than for the other annealed films.
منابع مشابه
Test structures for dielectric spectroscopy of thin films at microwave frequencies
This work describes the application of two different test structures to execute broadband microwave measurements of the dielectric constant of ceramic thin films. Coplanar waveguide probes and vector network analyzer were used to measure the dielectric constant versus frequency of thin films of lead zirconate titanate and zirconium titanate, fabricated by sol gel methods. One-step lithography w...
متن کاملProcessing Sol-gel Pzt Thin Films for Microactuators
Sol-gel derived lead zirconate titanate (PZT) thin films are being investigated for micromechanical applications. A synthesis technique which involves the spin coating of several thin layers followed by rapid thermal annealing to crystallize the perovskite phase and repetition to achieve thicker films is described. Methods of improving the PZT-PZT interfaces between subsequently annealed layers...
متن کاملEffect of Film Thickness on the Piezoelectric Properties of Lead Zirconate Titanate Thick Films Fabricated by Aerosol Deposition
Lead zirconate titanate (PZT) thick films with uniformly dispersed submicrometer pores were successfully fabricated on platinized silicon substrates with various thicknesses ranging from 1 lm to over 100 lm by aerosol deposition. Mixed powders of PZT and polyvinylidene fluoride (PVDF) were deposited for initial fabrication of composite films. After burn-out of the PVDF phase from the composite ...
متن کاملPhotochemical growth of silver nanoparticles on c(-) and c(+) domains on lead zirconate titanate thin films.
The photochemical growth of silver nanoparticles on the negative domains of lead zirconate titanate thin films is reported. A sample of highly [100] orientated lead zirconate titanate, with a ratio of 30:70, that was 65-70 nm thick grown on Pt-coated MgO was poled by use of piezoresponse force microscopy to produce defined regions of surface positive and negative polarization. A comparison betw...
متن کاملA Fully Integrated Materials Framework for Enabling the Wireless Detection of Micro-defects in Aging
NOTICES Disclaimers The findings in this report are not to be construed as an official Department of the Army position unless so designated by other authorized documents. Citation of manufacturer's or trade names does not constitute an official endorsement or approval of the use thereof. Destroy this report when it is no longer needed. Do not return it to the originator. Approved for public rel...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید
ثبت ناماگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودعنوان ژورنال:
- Nanotechnology
دوره 18 39 شماره
صفحات -
تاریخ انتشار 2007