Localized concentration reversal of lithium during intercalation into nanoparticles

نویسندگان

  • Wei Zhang
  • Hui-Chia Yu
  • Lijun Wu
  • Hao Liu
  • Aziz Abdellahi
  • Bao Qiu
  • Jianming Bai
  • Bernardo Orvananos
  • Fiona C Strobridge
  • Xufeng Zhou
  • Zhaoping Liu
  • Gerbrand Ceder
  • Yimei Zhu
  • Katsuyo Thornton
  • Clare P Grey
  • Feng Wang
چکیده

Nanoparticulate electrodes, such as Li x FePO4, have unique advantages over their microparticulate counterparts for the applications in Li-ion batteries because of the shortened diffusion path and access to nonequilibrium routes for fast Li incorporation, thus radically boosting power density of the electrodes. However, how Li intercalation occurs locally in a single nanoparticle of such materials remains unresolved because real-time observation at such a fine scale is still lacking. We report visualization of local Li intercalation via solid-solution transformation in individual Li x FePO4 nanoparticles, enabled by probing sub-angstrom changes in the lattice spacing in situ. The real-time observation reveals inhomogeneous intercalation, accompanied with an unexpected reversal of Li concentration at the nanometer scale. The origin of the reversal phenomenon is elucidated through phase-field simulations, and it is attributed to the presence of structurally different regions that have distinct chemical potential functions. The findings from this study provide a new perspective on the local intercalation dynamics in battery electrodes.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Nanoporous Ag-CNTs foamed electrode for lithium intercalation

Intercalation of lithium into Ag-CNTs sample is reported here. We have used a nano-porous silver foam as a frame for deposition of the CNTs   inside   the   pores   by   electrophoresis   deposition   (EPD) technique. By using  chronopotentiometry method,  we  have noticed that the Li storage capacity of the prepared Ag-CNTs electrode was improved  noticeably  in  comparison  with  literature. ...

متن کامل

Thermodynamics of Lithium Intercalation into Graphites and Disordered Carbons

The temperature dependence of the open-circuit potential of lithium half-cells was measured for electrodes of carbon materials having different amounts of structural disorder. The entropy of lithium intercalation, DS , and enthalpy of intercalation, DH , were determined over a broad range of lithium concentrations. For the disordered carbons, DS is small. For graphite, an initially large DS dec...

متن کامل

Atomic layer deposition of Al2O3 on V2O5 xerogel film for enhanced lithium-ion intercalation stability

V2O5 xerogel films were fabricated by casting V2O5 sols onto fluorine-doped tin oxide glass substrates at room temperature. Five, ten and twenty atomic layers of Al2O3 were grown onto as-fabricated films respectively. The bare film and Al2O3-deposited films all exhibited hydrous V2O5 phase only. Electrochemical impedance spectroscopy study revealed increased surface charge-transfer resistance o...

متن کامل

Numerical Simulation of Intercalation-Induced Stress in Li-Ion Battery Electrode Particles

Severe, particle-level strains induced during both production and cycling have been putatively linked to lifetime limiting damage in lithium-ion cells. Because of the presently unknown contributions of manufacturing and intercalation induced stresses in Li cells, this correlation is critical in determining optimal materials and manufacturing methods for these cells. Both global and localized lo...

متن کامل

Electrodeposition of Ag nanoparticles onto bamboo-type TiO2 nanotube arrays to improve their lithium-ion intercalation performance

Bamboo-type TiO2 nanotube arrays prepared via anodic oxidation are modified with Ag nanoparticles by pulsed electrochemical deposition, for improved lithium-ion intercalation property as the anode material in lithium-ion batteries. Heat treatment converts as-formed nanotubes into anatase for Ag deposition. Bare and Ag-modified nanotubes are cycled at a current density of 800 μAcm between 1.0 an...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 4  شماره 

صفحات  -

تاریخ انتشار 2018