The corrosion of bronzes was examined in the context of single-acid versus mixed-acid (as in urban acid rain) solutions. Two bi-component bronzes (copper with either 3% Sn or 7% Sn) that closely represent those of historic artifacts were immersed for five weeks in conditions designed to replicate those experienced by statues and ornaments in cities where rainfall and humidity constantly produce an electrolyte layer on the surfaces of bronzes. Ions, acids, and particles of pollutants can dissolve in this layer, resulting in a variety of harsh corrosion processes. The kinetics of corrosion and the properties of the resulting patinas were monitored weekly by electrochemical impedance spectroscopy and open-circuit potential measurements. The sizes and appearances of the corrosion products were monitored and used to estimate the progress of the corrosion, whose crystalline structures were visualized using scanning electron microscopy with energy dispersive spectroscopy, identified by X-ray diffraction, and characterized by spectrocolorimetry. The electrochemical measurements demonstrated that greater damage (in terms of color change and corrosion product formation) did not correspond to deficiencies in protection. The mixed-acid solution did not corrode the bronzes, as would be expected from the additive effects of the single acids. The postulated mechanisms of metal dissolution appear to be specific to a particular bronze alloy, with the tin component playing an important role.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Experimental Studies of Water Wetting in Large-Diameter Horizontal Oil/Water Pipe Flows

Internal pipeline corrosion in oil production and transportation is always associated with the presence of water, and the likelihood of corrosion generally increases with the volume fraction of water. When the walls of the pipeline are wetted with oil no corrosion is possible. Highly turbulent flow was associated with negligible corrosion due to water entrainment by the flowing oil, whereas low...

متن کامل

Corrosion Inhibition of Mild Steel in Acidic Solution by Apricot Gum as a Green Inhibitor

The inhibitive effect of apricot gum AG on mild steel in 0.5 M phosphoric acid solution was investigated by potentiodynamic polarization, electrochemical impedance spectroscopy EIS, linear polarization resistance and electrochemical noise EN techniques. The inhibition efficiency increased with increasing AG concentration up to a certain value and decreased with increasing temperature. Polarizat...

متن کامل

Berberis Aristata: A Highly Efficient and Thermally Stable Green Corrosion Inhibitor for Mild Steel in Acidic Medium

Plant extracts are extensively researched as a source of green corrosion inhibitors. Herein, we report on a highly efficient and thermally stable corrosion inhibitor from the stem extract of high-altitude shrub Berberis aristata. The corrosion inhibition efficiency (IE) of the extract was tested in 1.0 M H2SO4 for the corrosion protection of mild steel (MS) by using gravimetric and electrochemi...

متن کامل

THE EFFECT OF CRYOLITE NA3ALF6 AND SODIUM FLUORIDE NAF ON THE CORROSION AND WETTING BY MOLTEN AL-SI ALLOY OF ANDALUSITE BASED REFRACTORIES

In order to improve the corrosion resistance of aluminosilicate refractories by molten aluminum, alkaline fluoride NaF and cryolite Na3AlF6 powders were studied. Both physical and chemical properties are known to influence wetting and corrosion behavior. This paper devoted to determine the influence of alkaline fluoride and cryolite added to andalusite based castable on the reaction with a...

متن کامل

ELECTROCHEMICAL INVESTIGATION OF INHIBITORY OF NEW SYNTHESIZED TETRAZOLE DERIVATIVE ON CORROSION OF STAINLESS STEEL 316L IN ACIDIC MEDIUM

In this study, an  organic compound  inhibitor, namely N-benzyl-N-(4-chlorophenyl)-1H-tetrazole-5-amine (NBTA), was synthesized and the role of this inhibitor for corrosion protection of stainless steel (SS) exposed to 0.5 M H2SO4 was investigated using electrochemical, and quantum analysis. By taking advantage of potentiodynamic polarization, the inhibitory action of NBTA was found t...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره 7  شماره 

صفحات  -

تاریخ انتشار 2014