Analysis of the stability of 3Y-TZP zirconia abutments after thermocycling and mechanical loading

نویسندگان

  • Paulo J. Almeida
  • Cesar L. Silva
  • Jorge L. Alves
  • Filipe S. Silva
  • Ramiro C. Martins
  • João Sampaio-Fernandes
چکیده

Objectives: Although implant abutments made of yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) show great predictability, some issues related to its aging require further study. The objective of this in vitro study is to assess the stability of 3Y-TZP zirconia implant abutments with two different implant connections when subjected to aging simulation through thermocycling and mechanical loading (TCML). Methods: Ten 3Y-TZP zirconia abutments were selected and equally divided into two groups (n = 5): CEZr, abutments for externally hexed implants; and CIZr, abutments for implants with an internal conical connection. The samples were subjected to thermocycling (5000 cycles; 5–55 ◦C) and mechanical loading (1.2 × 106 cycles; 88.8 N; 4 Hz). Before and after the aging procedures, X-ray diffraction (XRD) analysis was conducted to observe tetragonalmonoclinic (t-m) phase transformation, and topographic surface analysis was performed by 3D profilometry, and data were analyzed using Mann-Witney test (p < 0.05). Results: XRD measurements revealed no monoclinic phase in any of the abutments after aging. The comparative analysis regarding roughness (using the Sa parameter) at the abutments’ seating platforms (using 3D profilometry) revealed a slight increase in roughness in both connections after TCML. Statistically significant differences (test U = 57.0, p = 0.161 > 0.05), before and after TCML, and between implants connections (test U = 57.0, p = 0.053 > 0.05) were not detected. Conclusions: After a 5-year simulation of its clinical use, the analyzed 3Y-TZP zirconia abutments did not show signs of aging. The connection’s geometry does not interfere in aging. © 2016 Sociedade Portuguesa de Estomatologia e Medicina Dentária. Published by Elsevier España, S.L.U. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/). ∗ Corresponding author. E-mail address: [email protected] (P.J. Almeida). http://dx.doi.org/10.1016/j.rpemd.2016.07.003 1646-2890/© 2016 Sociedade Portuguesa de Estomatologia e Medicina Dentária. Published by Elsevier España, S.L.U. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/). Document downloaded from http://www.elsevier.es, day 29/07/2017. This copy is for personal use. Any transmission of this document by any media or format is strictly prohibited.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparative analysis of the wear of titanium/ titanium and titanium/zirconia interfaces in implant/abutment assemblies after thermocycling and mechanical loading

Objectives: Due to its hardness, zirconia abutments may damage the titanium of the implant’s connection during its clinical use. This study aimed to assess the wear of the seating platforms of externally hexed titanium implants when connected to zirconia abutments comparing to titanium abutments, after thermocycling and mechanical loading (TCML). Methods: Six BNT® S4 external connection implant...

متن کامل

On the bulk degradation of yttria-stabilized nanocrystalline zirconia dental implant abutments: an electron backscatter diffraction study

Degradation of yttria-stabilized zirconia dental implants abutments due to the tetragonal to monoclinic phase transformation was studied in detail by microstructural characterization using Electron Back Scatter Diffraction (EBSD). The amount and distribution of the monoclinic phase, the grain-size distribution and crystallographic orientations between tetragonal and monoclinic crystals in 3 mol...

متن کامل

Low-temperature degradation of different zirconia ceramics for dental applications.

The aim of this investigation was to determine the influence of simulated ageing on the tetragonal-to-monoclinic phase transformation and on the flexural strength of a 3Y-TZP ceramic, compared to alumina toughened zirconia (ATZ) and ceria-stabilized zirconia (12Ce-TZP). Standardized disc specimens of each material were hydrothermally aged in steam at 134°C and 3bar for 0, 16, 32, 64 or 128h. Th...

متن کامل

Evaluation of the Effect of Zirconia and Titanium Abutments on Microleakage of Implant-Abutment Interface Under Oblique Cyclic Loading In Vitro

Background and Aim: Oral bacteria can proliferate in the implant-abutment interface (IAI) and cause inflammation in the peri-implant tissues and adjacent bone. This study aimed to assess the effect of zirconia and titanium abutments on the microleakage of the IAI under oblique cyclic loading conditions. Materials and Methods: In this in-vitro study, 12 implant-abutment assemblies with zirconia...

متن کامل

Comparative Evaluation of Microgap at the Interface of Titanium and Zirconium Abutments Following Oblique Cyclic Loading: An in vitro Study

Abstract   Background and Aim : Microgap in the implant-abutment interface is one of the main challenges in the treatment of two-piece implants. This study aimed to investigate the effect of two types of abutments (zirconia and titanium) on microgap at implant-abutment interface area under oblique cyclic loading in vitro. Methods and Materials In this in vitro study, 12 implant-abutment assemb...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2016