Preparation and Application of Immobilized Surfactant-Modified PANi-CNT/TiO2 under Visible-Light Irradiation
نویسندگان
چکیده
Hydrothermally and sol-gel-synthesized immobilized surfactant-modified polyaniline-carbon nanotubes/TiO₂ (PANi-CNT/TiO₂) photocatalysts were prepared and their application in the degradation of diethyl phthalate (DEP) under visible light at 410 nm was investigated in this sturdy. To improve the dispersion of nanoparticles and the transfer of electrons, the TiO₂ surface was modified with both sodium dodecyl sulfate (SDS) and functionalized carbon nanotubes (CNT-COOH and CNT-COCl). With the addition of PANi, which was increased from 1%-5%, the adsorption edge of the prepared photocatalysts shifted to 442 nm. The SDS linked the PANi polymers to achieve a thickness of coating of the film of up to 314-400 nm and 1301-1600 nm for sol-gel hydrolysis and hydrothermally-synthesized photocatalysts, respectively. An appropriate film thickness would extend the transfer path of the electrons and inhibit the recombination of the electrons and the electron-holes. The photo-degradation performance of DEP by the hydrothermally-synthesized photocatalysts was better than those by sol-gel hydrolysis. The results revealed that the hydroxyl radicals were the key oxidant in the degradation of DEP using hydrothermally-synthesized PANi-CNT/TiO₂ photocatalysts. The morphology and functional groups of the raw materials of photocatalysts were characterized and a comparison of photocatalytic activity with other TiO₂-based photocatalysts was also provided.
منابع مشابه
Comparison of Photocatalytic Activities of Two Different Dyes Using Pt-Modified TiO2 Nanoparticles under Visible Light
The photocatalytic degradation of Acid Red 91 (AR91) and Acid Yellow 23 (AY23) with different molecular structures and different substitute groups using Pt modified TiO2 (PtTiO2 ) nanoparticles was investigated in the presence of visible light irradiation. Pt-TiO2 nanoparticles were prepared with photodiposition method (PD) and characterized by X-ray diffraction (XRD), scanning electron microgr...
متن کاملUpgrading TiO2 Photoactivity under Visible Light by Synthesis of MWCNT/TiO2 Nanocomposite
Nanocomposites of multi-walled carbon nanotubes and titanium dioxide (MWCNT/TiO2) were synthesized by the sol-gel method. Regarding hydrophobicity of carbon nanotubes (CNTs), benzyl alcohol was used as the linking agent between CNT powder and TiO2 gel which was prepared from the precursor of titanium tetraisopropoxide. The prepared samples were treated under thermal treatments. A part of the sa...
متن کاملAg-doped TiO2 Nanocomposite Prepared by Sol Gel Method: Photocatalytic Bactericidal Under Visible Light and Characterization
In this reaserch, photocatalyst titanium dioxide was doped with silver and modified by polyethylene glycol by sol gel method and the samples were characterized by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The purpose of the present study was to evaluate the photocatalytic bactericidal effects of prepared nanocomposite on human p...
متن کاملAntibacterial response of Cd-TiO2/PEG/folic acid nanocomposite under ultraviolet, visible light, or ultrasonic irradiation
Synthesis and characterization of Cd-TiO2/PEG/FA nanocomposite as a biomaterial is the main aim of this research. Cd-doped TiO2 nanoparticles (NPs) were synthesized by solvothermal assisted sol-gel method. Then, polyethylene glycol (PEG) was added to the as-synthesized NPs in order to modify their surface and to prevent agglomeration. In the next step, folic acid (FA) was conjugated to Cd-TiO2/...
متن کاملPhotocatalytic degradation of methyl orange using TiO2:Mg2+/zeolite composite under visible light irradiation
Photodegradation of methyl orange was investigated using synthesized TiO2:Mg2+/zeolite as the photocatalyst. The photocatalyst was characterized by X-ray, XRF, FT-IR, and SEM. The photocatalytic activities of TiO2:Mg2+/zeolite samples were evaluated in the degradation of methyl orange under visible light irradiation. The appropriate content of Mg in the composite was obtained as 4.711 wt% with ...
متن کامل