Formation mechanisms for the dominant kinks with different angles in InP nanowires
نویسندگان
چکیده
The morphologies and microstructures of kinked InP nanowires (NWs) prepared by solid-source chemical vapor deposition method were examined using scanning electron microscopy (SEM) and high-resolution transmission electron microscopy (HRTEM). Statistical analysis and structural characterization reveal that four different kinds of kinks are dominant in the grown InP NWs with a bending angle of approximately 70°, 90°, 110°, and 170°, respectively. The formation mechanisms of these kinks are discussed. Specifically, the existence of kinks with bending angles of approximately 70° and 110° are mainly attributed to the occurrence of stacking faults and nanotwins in the NWs, which could easily form by the glide of {111} planes, while approximately 90° kinks result from the local amorphorization of InP NWs. Also, approximately 170° kinks are mainly caused by small-angle boundaries, where the insertion of extra atomic planes could make the NWs slightly bent. In addition, multiple kinks with various angles are also observed. Importantly, all these results are beneficial to understand the formation mechanisms of kinks in compound semiconductor NWs, which could guide the design of nanostructured materials, morphologies, microstructures, and/or enhanced mechanical properties.
منابع مشابه
Improving the optical properties of thin film plasmonic solar cells of InP absorber layer using nanowires
In this paper, a thin-film InP-based solar cell designed and simulated. The proposed InP solar cell has a periodic array of plasmonic back-reflector, which consists of a silver layer and two silver nanowires. The indium tin oxide (ITO) layer also utilized as an anti-reflection coating (ARC) layer on top. The design creates a light-trapping structure by using a plasmonic back-reflector and an an...
متن کاملSoluble InP and GaP nanowires: self-seeded, solution-liquid-solid synthesis and electrical properties.
A facile, self-seeded, solution-liquid-solid growth of soluble InP and GaP nanowires with a very low amount of native point defects with respect to the carrier concentrations have been synthesized (see scheme) and characterized. They are potentially promising building blocks in optoelectronic applications.We demonstrate a facile method for self-seeded, solution-liquid-solid growth of soluble In...
متن کاملHydrazine-Assisted Formation of Indium Phosphide (InP)-Based Nanowires and Core-Shell Composites
Indium phosphide nanowires (InP NWs) are accessible at 440 °C from a novel vapor phase deposition approach from crystalline InP sources in hydrazine atmospheres containing 3 mol % H₂O. Uniform zinc blende (ZB) InP NWs with diameters around 20 nm and lengths up to several tens of micrometers are preferably deposited on Si substrates. InP particle sizes further increase with the deposition temper...
متن کاملنقش ناهمسانگردیهای بلوری و شکلی بر خواص مغناطیسی نانوسیمهای کبالت و نیکل
Co and Ni magnetic nanowires with different diameter and deposition time were fabricated into the alumina template using ac electrodeposition. For Ni nanowires with 30 nm diameter the coercivity initially increased then dropped with deposition time, while it only increased with deposition time for all the other diameters. In general, the results showed that the coercivity reduced with diamete...
متن کاملDiameter Dependence of Planar Defects in InP Nanowires
In this work, extensive characterization and complementary theoretical analysis have been carried out on Au-catalyzed InP nanowires in order to understand the planar defect formation as a function of nanowire diameter. From the detailed transmission electron microscopic measurements, the density of stacking faults and twin defects are found to monotonically decrease as the nanowire diameter is ...
متن کامل