The effect of thermocycling on the bonding of different restorative materials to access opening through porcelain fused to metal restorations
نویسندگان
چکیده
PURPOSE Porcelain fused to metal (PFM) crowns provide the best treatment option for teeth that have a large or defective restoration. More than 20% of teeth with PFM crowns or bridges require non-surgical root canal treatment (NSRCT). This may be due to the effect of restorative procedures and the possible leakage of bacteria and or their by-products, which leads to the demise of the tooth pulp. Thus, this study was planned to compare the ability of the restorative materials to seal perforated PFM specimens. MATERIALS AND METHODS The study evaluates the ability of amalgam, composite or compomer restorative materials to close perforated PFM specimen's in-vitro. Ninety PFM specimens were constructed using Ni-Cr alloys and feldspathic porcelain, and then they were divided into 3 groups: amalgam (A), composite + Exite adhesive bond (B) and compomer + Syntac adhesive bond (C). All the PFM samples were embedded in an acrylic block to provide complete sealing of the hole from the bottom side. After the aging period, each group was further divided into 3 equal subgroups according to the thermocycling period (one week for 70 cycles, one month for 300 cycles and three months for 900 cycles). Each subgroup was put into containers containing dye (Pelikan INK), one maintained at 5℃ and the other at 55℃, each cycle for 30 sec time. The data obtained was analyzed by SPSS, 2006 using one way ANOVA test and student t-test and significant difference level at (P<.01). RESULTS The depth of dye penetration was measured at the interfaces of PFM and filling materials using Co-ordinate Vernier Microscope. The lowest levels of the dye penetration for the three groups, as well as subgroups were during the first week. The values of dye leakage had significantly increased by time intervals in subgroups A and C. CONCLUSION It was seen that amalgam showed higher leakage than composite while compomer showed the lowest level of leakage.
منابع مشابه
Evaluation of thermocycling and cyclic loads on the amount of microleakage of resin bonded restorations
Evaluation of thermocycling and cyclic loads on the amount of microleakage of resin bonded restorations Dr. H. Siadat* - Dr. A. Mirfazaelian* - Dr. S. Mirmohammadrezaee* *- Assistant Professor of Removable Prosthodontics Dept. - Faculty of Dentistry – Tehran University of Medical Sciences. Background and Aim: Resin bonded restorations are preferred to the conventional ones due to their potentia...
متن کاملComparison of the Effect of Three methods of Porcelain Surface Treatment on Shear Bond Strength of Composite to Porcelain
Background and Aim: Several methods are available for intraoral repair of chipped porcelain restorations by composite resin. Also, there is still controversy regarding the best method of porcelain repair in terms of bond strength and cost effectiveness. This study aimed to compare three methods of porcelain surface treatment on shear bond strength (SBS) of composite to porcelain. Materials a...
متن کاملAn evaluation of the marginal integrity of porcelain fused to base metal crowns after extension of porcelain to the border of the margin
An evaluation of the marginal integrity of porcelain fused to base metal crowns after extension of porcelain to the border of the margin Dr. Sh. Rokni* - Dr. M. Seifi** - Dr. A. Eizadi *** *- Professor & Head of Prosthodontics Dept. Faculty of Dentistry – Mashhad University of Medical Sciences. **- Assistant Professor of Prosthodontics Dept. Faculty of Dentistry – Mashhad University of Medical ...
متن کاملEffect of Thermocycling and Type of Restorative Material on Microleakage of Class II Restorations
Objectives: Microleakage is a major cause of failure of dental restorations and results in development of secondary caries, tooth hypersensitivity and pulp pathosis. This study aimed to compare the microleakage of class II cavities filled with two types of composite resins and a compomer and subjected to thermocycling. Methods: In this in vitro experimental study, class II cavities with a gi...
متن کاملThe Effect of Dental Bonding Agent of Excite on the Rate of Microleakage in Class V Amalgam Restorations
Aim: This study was done to evaluate the rate of microleakage in class V amalgam restorations in which the dental bonding agent (DBA) Excite was used as a sealer beneath the restorations. Methods: four amalgam restorative materials with commercial names of Dentam, Cinalux, Tytin and SDI (GS-80) were used. Seventy sound human premolars were selected and randomly divided into 4 groups of 15 teeth...