On the initiation of cyclic oxidation-induced rumpling of platinum-modified nickel aluminide coatings
نویسندگان
چکیده
The evolution of the surface roughness of an initially flat platinum-modified nickel aluminide (NiPtAl) coating on a single crystal superalloy with cyclic oxidation has been measured by optical profilometry and correlated with the aluminide microstructure. The roughness evolution is dominated by the relative motion of individual grains on thermal cycling, with the larger sized grains moving up and the smaller grains moving down with respect to the average surface. Detailed crystallographic analysis indicates that the grains in the coating are randomly distributed and have no crystallographic relationship with the underlying single crystal superalloy. Furthermore, there is a correlation between the number of sides a grain has and the propensity for its center to move relative to the average surface plane: grains with six or more sides bow up, whereas the surfaces of those grains with fewer than six sides bow down. It is proposed that rumpling initiates due to the vertical displacement of the smaller grains having fewer than six sides. Once initiated, rumpling proceeds driven by the strain energy in the thermally grown oxide. 2009 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
منابع مشابه
Nickel Base Superalloy Rene®80 – The Effect of High Temperature Cyclic Oxidation on Platinum-Aluminide Coating Features
Nickel base superalloy alloys are used in the manufacture of gas turbine engine components, which in use are exposed to high temperatures and corrosive environments. The platinum aluminide coatings described here have been developed to protect nickel base superalloy alloys from oxidation. In this study, the effect of cyclic oxidation, platinum layer thickness and aluminizing process on beha...
متن کاملEffect of superimposed uniaxial stress on rumpling of platinum-modified nickel aluminide coatings
Thermal cycling of a platinum modified, nickel aluminide (Ni,Pt)Al coated single crystal superalloy, between 1000 and 1150 C with 10 min holds at each temperature, and subject to a compressive uniaxial stress is reported. There are two major effects of the superimposed compressive stress not observed in the absence of the stress. One is that the rumpling pattern exhibits an asymmetry with an in...
متن کاملCyclic oxidation-induced cracking of platinum-modified nickel-aluminide coatings
Short cracks, extending to the interdiffusion zone, have been observed in platinum-modified nickel-aluminide diffusion coatings on single-crystal CMSX-4 superalloys after these have been subject to short (10 min) rapid thermal cycles. The cracks were revealed after removing the thermally grown oxide formed during cycling on the coating surfaces. Cracking was observed for coatings subject to the...
متن کاملFormation and Evaluation of Oxidation Behavior of Zirconia- Aluminide Coating on Nickel- Based Alloy
Practical applications of thermal barrier coatings with aluminide bond-coats are limited due to oxide scale spallation of the aluminide coating under applied thermal stresses. Considering the positive effects of oxygen-active elements or their oxides on the high temperature oxidation behavior, in this research zirconia was introduced into an aluminide coating. For this purpose, a Watts type bat...
متن کاملCyclic oxidation behavior of uncoated and aluminum-rich nickel aluminide coated Rene-80 superalloy
In this study, aluminide coating was employed to enhance the high-temperature cyclic oxidation of Rene-80 superalloy at 950ºC. The microstructural aspects and phase constituents of samples were investigated with scanning electron microscopy (SEM) and x-ray diffraction (XRD) techniques. The result of oxidation tests showed that the weight gain in the uncoated sample was considerably higher than...