Failure Modes in Ceramic-Based Layer Structures: A Basis for Materials Design of Dental Crowns

نویسندگان

  • Brian Lawn
  • Sanjit Bhowmick
  • Mark B. Bush
  • Tarek Qasim
  • Yu Zhang
چکیده

A research program on failure modes induced by spherical indenters in brittle layer structures bonded to polymeric substrates, in simulation of occlusal function in all-ceramic dental crowns, is surveyed. Tests are made on model flat and curved layers bonded onto a dentin-like polymer base, in bilayer (ceramic/polymer) and trilayer (ceramic/ceramic/polymer) configurations. All-transparent systems using glass as a porcelain-like outer or veneer layer and sapphire as a stiff and strong core support layer enable in situ observation of the entire evolution of fracture modes in the brittle layers, from initiation through to failure. With the fracture modes identified, tests are readily extended to systems with opaque polycrystalline dental core ceramics, notably alumina and zirconia. A variety of principal failure modes is identified: outer and inner cone cracks developing in the near-contact region at the top surface; radial cracks developing at the bottom surface along the loading axis; margin cracks from the edges of dome-like structures. All of these modes are exacerbated in cyclic loading by time-cumulative slow crack growth, but inner cones are subject to especially severe mechanical fatigue from hydraulic pumping of water into the crack fissures. Conditions under which each mode may be expected to dominate, particularly in relation to geometrical variables (layer thickness, contact radius) and relative material properties, are outlined. Clinical issues such as crown geometry, overload versus fatigue failure, role of residual stresses in fabrication, etc. are addressed.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fracture of ceramic/ceramic/polymer trilayers for biomechanical applications.

Fracture damage in trilayers consisting of outer and inner brittle layers bonded to a compliant (polycarbonate) substrate and subjected to concentrated surface loading is analyzed. The principal mode of fracture is radial cracking at the undersurface of the inner (core) layer, even in the strongest of core ceramics--other damage modes, including radial cracking in the outer (veneer) layer, are ...

متن کامل

Simulation of clinical fractures for three different all-ceramic crowns

Comparison of fracture strength and fracture modes of different all-ceramic crown systems is not straightforward. Established methods for reliable testing of all-ceramic crowns are not currently available. Published in-vitro tests rarely simulate clinical failure modes and are therefore unsuited to distinguish between the materials. The in-vivo trials usually lack assessment of failure modes. F...

متن کامل

Dental ceramics and the molar crown testing ground.

All ceramic crowns are highly esthetic restorations and their popularity has risen with the demand for life-like and cosmetic dentistry. Recent ceramic research has concentrated on developing a fundamental understanding of ceramic damage modes as influenced by microstructure. Dental investigations have elucidated three damage modes for ceramic layers in the 0.5-2 mm thickness using point contac...

متن کامل

Monolithic CAD/CAM lithium disilicate versus veneered Y-TZP crowns: comparison of failure modes and reliability after fatigue.

PURPOSE The aim of this research was to evaluate the fatigue behavior and reliability of monolithic computer-aided design/computer-assisted manufacture (CAD/CAM) lithium disilicate and hand-layer-veneered zirconia all-ceramic crowns. MATERIALS AND METHODS A CAD-based mandibular molar crown preparation, fabricated using rapid prototyping, served as the master die. Fully anatomically shaped mon...

متن کامل

Contact fracture of full-ceramic crowns subjected to occlusal loads.

The mechanisms contributing to failure of full dental ceramic crowns under occlusal loads were studied using a unique optical approach. Model specimens comprising triple-layered crowns (veneer, core and substrate) were developed with both flat and curved occlusal surfaces and then subjected to simulated quasi-static occlusal loading using a spherical indenter. Deformation within the specimens d...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2007