The light output, α/β ratio, and pulse shape have been investigated at −25◦ C with PbWO4 crystal scintillators undoped, and doped by F, Eu, Mo, Gd and S. The fast 0.01 − 0.06 μs and middle 0.1 − 0.5 μs components of scintillation decay were observed for all the samples. Slow components of scintillation signal with the decay times 1− 3 μs and 13− 28 μs with the total intensity up to ≈ 50% have been recognized for several samples doped by Molybdenum. We found some indications of a pulse-shape discrimination between α particles and γ quanta with PbWO4 (Mo doped) crystal scintillators.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

PULSE SHAPE DISCRIMINATION CHARACTERISTICS OF STILBENE CRYSTAL, EJ-299-33 AND Li LOADED PLASTIC SCINTILLATORS FOR A HIGH RESOLUTION CODED-APERTURE NEUTRON IMAGER

Pulse shape discrimination performances of single stilbene crystal, EJ-299-33 plastic and Li loaded plastic scintillators have been compared. Pulse Gradient Analysis pulse shape discrimination algorithm has been tested for each scintillator sample, assessing their neutron/gamma separation. In this study each scintillator sample was irradiated with a Cf neutron source and, a real-time fast digit...

متن کامل

Further study of CdWO4 crystal scintillators as detectors for high sensitivity 2β experiments: scintillation properties and pulse-shape discrimination

Energy resolution, light yield, non-proportionality in the scintillation response, α/β ratio, pulse shape for γ rays and α particles were studied with CdWO4 crystal scintillators. Some indication for a difference in the emission spectra for γ rays and α particles was observed. No dependence of CdWO4 pulse shape on emission spectrum wavelengths under laser, α particles and γ ray excitation was o...

متن کامل

Pulse-shape discrimination of La halide scintillators

The bright scintillators LaCl3:Ce and LaBr3:Ce were tested for a–g pulse-shape discrimination (PSD). PSD is demonstrated for LaCl3:Ce but not for LaBr3:Ce: r 2005 Elsevier B.V. All rights reserved.

متن کامل

Measurements of Separate Neutron and Gamma-Ray Coincidences with Liquid Scintillators and Digital Pulse Shape Discrimination

..................................................................................................................... vii

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2008