Durability of anti-graffiti coatings on stone: natural vs accelerated weathering
نویسندگان
چکیده
Extending the use of novel anti-graffiti coatings to built heritage could be of particular interest providing the treatments are efficient enough in facilitating graffiti removal and long-lasting to maintain their protective properties without interfering with the durability of the substrates. However, studies of the durability of these coatings are scarce and have been mainly carried out under accelerated weathering conditions, the most common practice for assessing the durability of materials but one that does not reproduce accurately natural working conditions. The present study aimed to assess the durability of the anti-graffiti protection afforded by two anti-graffiti treatments (a water dispersion of polyurethane with a perfluoropolyether backbone and a water based crystalline micro wax) on Portland limestone and Woodkirk sandstone after 1 year of outdoor exposure in the South of England with periodic painting and cleaning episodes taking place. A parallel study under artificial weathering conditions in a QUV chamber for 2000 hours was also carried out. Changes to the coatings were assessed by measuring colour, gloss, water-repellency, roughness and microstructure, the latter through micro-Raman and optical microscope observations, periodically during the experiments. The results show that both anti-graffiti treatments deteriorated under both artificial and natural weathering conditions. For the polyurethane based anti-graffiti treatment, artificial ageing produced more deterioration than 1 year of outdoor exposure in the south of England due to loss of adhesion from the stones, whereas for micro wax coating there were no substantial differences between the two types of weathering.
منابع مشابه
Weathering of Two Anti-Graffiti Protective Coatings on Concrete Paving Slabs
The durability of anti-graffiti coatings is of special relevance since, unlike other protective treatments, they are not only affected by environmental factors, but also by often aggressive cleaning procedures. However, little is known about the long-term performance of either permanent or sacrificial coatings. This study explores the durability of two commercial coatings on concrete paving sla...
متن کاملInfluence of the Distribution of a Spray Paint on the Efficacy of Anti-Graffiti Coatings on a Highly Porous Natural Stone Material
Graffiti on facades often has a heavy impact in social and economic terms, particularly when historical and artistic artefacts are affected. To limit the damages to the surfaces, preventive plans are implemented and anti-graffiti coatings are used as a protective measure. In this study, the distribution of a spray paint inside a highly porous stone, with and without anti-graffiti protection, wa...
متن کاملPetrophysical and durability tests on sandstones for the evaluation of their quality as building stones using Analytical Hierarchy Process (AHP)
Due to their widespread availability, sandstones are commonly used as a natural stone for buildings, monuments and sculptures. In thecurrent study, nine sandstone samples from the Upper Red Formation (specified by the letters A, B, C, CG, S, S1, Sh, Tr and Min)were studied from a petrophysical point of view and their durability was evaluated. Then, their suitability as building stones wasassess...
متن کاملCOST E 18 – Contact Proforma
Special Equipment: Artificial weathering devices (several wheels and QUV, Global UV test system), natural exposure site. UV-visible spectrophotometer, IR spectrophotometer linked with a IR microscope, thermal analysis equipment (DSC), fluorescence microscope, chromatographical equipment, goniometer,…. Improvement of durability of coated wood (especially for transparent coatings) Study of the wo...
متن کاملEffect of Mineralogy on Durability and Strength of Hornfelsic Rocks under Acidic Rainfall in Urban Areas
In order to assess mineralogical composition influence on durability and strength of rocks, four samples of hornfelsic rocks were selected from southern and western parts of the city of Hamedan, west of Iran. These rock samples were subjected to mineralogical, physical and mechanical tests in the laboratory. Also, they were evaluated in 15 cycles of slake-durability testing in different pH of s...