Tetra­yttrium(III) tris­ulfide disilicate

نویسندگان

  • Lukasz A. Koscielski
  • James A. Ibers
چکیده

Tetra-yttrium(III) tris-ulfide disilicate, Y(4)S(3)(Si(2)O(7)), crystallizes in the Sm(4)S(3)(Si(2)O(7)) structure type. The structure consists of isolated (Si(2)O(7))(6-) units (2mm. symmetry) and two crystallo-graphically independent Y(3+) cations bridged by one S and one O atom. The first Y atom (site symmetry .m.) is coordinated by three O atoms and three S atoms in a trigonal-prismatic arrangement whereas the second Y atom (site symmetry ..2) is coordinated by six O atoms and three S atoms in a tricapped trigonal-prismatic arrangement.

منابع مشابه

Tetra­yttrium difluoride disilicate orthosilicate, Y4F2[Si2O7][SiO4]

In the crystal structure of Y4F2[Si2O7][SiO4], three fundamental building blocks are present, viz. anionic disilicate and orthosilicate units ([Si2O7](6-) and [SiO4](4-)) and cationic [F2Y4](10+) entities. The latter are built up by two [FY3](8+) triangles sharing a common edge. The four crystallographically independent Y(3+) cations display coordination numbers of eight for one and of seven fo...

متن کامل

Shear Bond Strength of Porcelain Veneering to Nickel-Chromium, Chromium-Cobalt, Zirconia and Lithium Disilicate

Background and Aim: High chipping rates of the veneering porcelain in zirconia ce-ramic restorations have been reported in many clinical studies. However, information on the bonding behavior of veneering porcelain to zirconia and lithium disilicate frameworks is limited. The purpose of this study was to evaluate the bond-ing strength of porcelain veneering to zirconia, lithium disilicate, nicke...

متن کامل

Comparison of Shear Bond Strengths of Conventional Resin Cement and Self-adhesive Resin Cement bonded to Lithium Disilicate: An in vitro Study.

AIM The aim of this study is to compare the shear bond strengths of conventional resin cement and self-adhesive resin cement bonded to lithium disilicate. MATERIALS AND METHODS A total of 40 extracted human molar teeth were mounted in self-cure acrylic resin. Teeth were prepared to obtain flat occlusal surface. About 40 lithium disilicate specimens of dimension-10 mm in diameter and thickness...

متن کامل

Shear bond strength of veneering ceramic to coping materials with different pre-surface treatments

PURPOSE Pre-surface treatments of coping materials have been recommended to enhance the bonding to the veneering ceramic. Little is known on the effect on shear bond strength, particularly with new coping material. The aim of this study was to investigate the shear bond strength of veneering ceramic to three coping materials: i) metal alloy (MA), ii) zirconia oxide (ZO), and iii) lithium disili...

متن کامل

Influence of cementation and cement type on the fracture load testing methodology of anterior crowns made of different materials.

To evaluate the influence of cementation on fracture load of anterior crowns made of CAD/CAM-resin-blocks (ART), leucite-reinforced glass-ceramics (LRG), lithium disilicate ceramics (LIT), veneered zirconia (ZRO) and veneered alloy (DEG). Each crown group (n=15/subgroup) was cemented on the metal abutment as follows: i. using glass ionomer, ii. using self-adhesive resin cement, and iii. not cem...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

متن کامل
عنوان ژورنال:

دوره 67  شماره 

صفحات  -

تاریخ انتشار 2011