statement of problem: recent clinical results for zirconia all-ceramic restorations have revealed that the fracture rate 6-15% of the zirconia framework is so low and the core of zirconia has high stability. however, chipping-off fractures of porcelain are the most common reason for failures of zirconia in the fixed partial dentures. objectives: the purpose of this study was to compare the shear bond strength (sbs) of porcelain in the porcelain fused to metal and all-ceramic crowns with zirconia core. materials and methods: two groups were selected: porcelain fused to metal (pfm) and porcelain fused to zirconia (pfz) (n = 30).in the pfm group, a wax model (10 × 10 × 10mm)was used to cast metal base (ni_cr alloy). in the pfz group, an acrylic cubic model (10 × 10 × 10mm) was made as zirconia model for scanning.15 cubic zirconia samples were milled by cad-cam. the procedure of porcelain veneering was conducted by the conventional layering technique up to 2 mm thickness (2.5 × 2.5 × 2 mm). all specimens were stored in water for 48 hrs. thermal cycling was conducted for 20000 cycles between 55°c and 5ºc alternatively for 30s.all samples were mounted in acrylic resin and the sbs test was performed, using a universal testing machine. the analysis of data was performed at a significance level of 0.05 using kolmogorov-smirnov and mann-whitney u-test. results: mean of sbs in pfm and pfz was 24.57 and 20.88, respectively. the results of mann-whitney test showed that there was no statistically significant difference between the two groups of porcelain fused to metal and zirconia in item shear bond strength ( p = 0.455). conclusions: there was no significant difference between the two groups of pfm and pfz in the item sbs.
منابع مشابه
Shear Bond Strength of Porcelain to a Base-Metal Compared to Zirconia Core
STATEMENT OF PROBLEM Recent clinical results for Zirconia all-ceramic restorations have revealed that the fracture rate 6-15% of the Zirconia framework is so low and the core of Zirconia has high stability. However, chipping-off fractures of porcelain are the most common reason for failures of Zirconia in the fixed partial dentures. OBJECTIVES The purpose of this study was to compare the shea...
متن کاملShear bond strength of veneering porcelain to porous zirconia.
In this study, two types of porous zirconia and dense zirconia were used. The flexural strength of non-layered zirconia specimens and those of the layered zirconia specimens with veneering porcelain were examined. Furthermore, the shear bond strength of veneering porcelain to zirconia was examined. The flexural strength of the non-layered specimens was 1,220 MPa for dense zirconia and 220 to 30...
متن کاملA Comparative Evaluation of Shear Bond Strength of Creation Ceramic Veneer to Metal and Zirconia Cores
Abstract Background and Aim: High chipping rates of the veneering porcelain of zirconia ceramic restorations have been reported in clinical studies. Thus, the shear bond strength (SBS) between the zirconia core and veneering porcelain requires investigation. Materials and Methods: In this in-vitro study, at first, using a computer-aided design/computer-aided manufacturing (CAD/CAM) machine, 1...
متن کاملShear Bond Strength of Porcelain Veneering to Nickel-Chromium, Chromium-Cobalt, Zirconia and Lithium Disilicate
Background and Aim: High chipping rates of the veneering porcelain in zirconia ce-ramic restorations have been reported in many clinical studies. However, information on the bonding behavior of veneering porcelain to zirconia and lithium disilicate frameworks is limited. The purpose of this study was to evaluate the bond-ing strength of porcelain veneering to zirconia, lithium disilicate, nicke...
متن کاملShear bond strength of veneering porcelain to zirconia and metal cores
STATEMENT OF PROBLEM Zirconia-based restorations have the common technical complication of delamination, or porcelain chipping, from the zirconia core. Thus the shear bond strength between the zirconia core and the veneering porcelain requires investigation in order to facilitate the material's clinical use. PURPOSE The purpose of this study was to evaluate the bonding strength of the porcela...
متن کاملShear Bond Strength of Metal brackets to Zirconia Treated with Er:YAG Laser Sandblasting and Silane
Background and Aim: Application of zirconia ceramics has increased. Since the commonly used surface treatment for porcelain, i.e. acid etching is not efficient for zirconia surfaces, evaluation of other surface treatment methods for zirconia is important. The aim of this study was to compare the shear bond strength (SBS) of metal brackets to zirconia treated with different powers of Er:YAG lase...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
عنوان ژورنال:
journal of dental biomaterialsجلد ۴، شماره ۱، صفحات ۳۶۷-۰
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023