effect of saliva on load-deflection characteristics of superelastic nickel-titanium orthodontic wires.

نویسندگان

t hosseinzadeh nik professor, department of orthodontics, faculty of dental research center and dentistry, tehran university of medical sciences, tehran, iran.

h ghadirian

m nili ahmadabadi

t shahhoseini

چکیده

most published results about the characteristics of niti wires are based on the mechanical laboratory tests on the as-received wires.the purpose of this study was to investigate the effect of saliva on load-deflection characteristics of superelastic niti wires.in this experimental study, 15 wires of three kinds of superelastic niti wires (sentalloy, force i and truflex) were prepared. five specimens of each wire were tested in the as-received condition (t0) to provide baseline information and the remaining wires were divided into two groups of five. half of them were kept inside artificial saliva for one month (t1), while the others were kept in air (t2). after 30 days, three-point bending test was done in a dental arch model and data from selected points on the unloading phase of the generated graphs were used for statistical analysis.force i and truflex showed significantly greater force than sentalloy. the load values of truflex and force i after one month exposed to artificial saliva (t1) decreased significantly, but sentalloy was not affected significantly. the plateau gap values were not considerably different among t0, t1 and t2.saliva decreased the load of force i and truflex significantly, but it did not have a statistically significant effect on sentalloy.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Saliva on Load-Deflection Characteristics of Superelastic Nickel-Titanium Orthodontic Wires

OBJECTIVE Most published results about the characteristics of NiTi wires are based on the mechanical laboratory tests on the as-received wires.The purpose of this study was to investigate the effect of saliva on load-deflection characteristics of superelastic NiTi wires. MATERIALS AND METHODS In this experimental study, 15 wires of three kinds of superelastic NiTi wires (Sentalloy, Force I an...

متن کامل

Load-deflection characteristics of superelastic nickel-titanium wires.

OBJECTIVE To determine the mechanical properties of commercially available thermodynamic wires and to classify these wires mathematically into different groups. MATERIALS AND METHODS The samples examined were 48 nickel-titanium (NiTi) alloy orthodontic wires commercially available from five manufacturers. These samples included 0.016-inch, 0.016- x 0.022-inch, 0.017- x 0.025-inch, and 0.018- ...

متن کامل

The effect of fluoride exposure on the load-deflection properties of superelastic nickel-titanium-based orthodontic archwires.

BACKGROUND It has been demonstrated that fluoride prophylactic agents may cause hydrogen absorption in NiTi wires and degrade their mechanical properties. AIMS To investigate the effect of a fluoride mouthwash on load-deflection characteristics of three types of nickel-titanium-based orthodontic archwires. METHODS Twenty maxillary 0.016 inch round specimens from each of the single-strand Ni...

متن کامل

Deflection load characteristics of laser-welded orthodontic wires.

OBJECTIVE To compare the deflection load characteristics of homogeneous and heterogeneous joints made by laser welding using various types of orthodontic wires. MATERIALS AND METHODS Four kinds of straight orthodontic rectangular wires (0.017 inch × 0.025 inch) were used: stainless-steel (SS), cobalt-chromium-nickel (Co-Cr-Ni), beta-titanium alloy (β-Ti), and nickel-titanium (Ni-Ti). Homogene...

متن کامل

Load Deflection Characteristics of Nickel Titanium Initial Archwires.

OBJECTIVES The aim of this study was to assess and compare the characteristics of commonly used initial archwires by their load deflection graphs. MATERIALS AND METHODS This study tested three wire designs namely copper nickel titanium (CNT), nickel titanium (NiTi), and multi-strand NiTi (MSNT) archwires engaged in passive self-ligating (PSL) brackets, active self-ligating (ASL) brackets or c...

متن کامل

load deflection characteristics of nickel titanium initial archwires

objectives: the aim of this study was to assess and compare the characteristics of commonly used initial archwires by their load deflection graphs. materials and methods : this study tested three wire designs namely copper nickel titanium (cnt), nickel titanium (niti), and multi-strand niti (msnt) archwires engaged in passive self-ligating (psl) brackets, active self-ligating (asl) brackets or ...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید


عنوان ژورنال:
journal of dentistry, tehran university of medical sciences

جلد ۹، شماره ۴، صفحات ۱۷۱-۹

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023