in this investigation the thickness of enamel in the gingival, middle, and incisal thirds of the labial surface of the anterior teeth were measured regarding preparation of the teeth for porcelain laminate veneers.part one, 20 extracted intact human maxillary central and lateral incisors ten of each were selected. the teeth were imbedded in autopolimerize acrylic resin. cross section was preformed through the midline of the incisal, middle and cervical one-third of the labial surface of the teeth. the samples were observed under reflected stereomicroscope and the thickness of enamel was recorded. part ii, the effect of different types of preparation on dentin exposure was evaluated. thirty maxillary central incisor teeth were randomly divided into two groups: a: knife-edge preparation. b: chamfer preparation. all samples were embedded in autopolimerize acrylic resin using a silicon mold. the samples were cut through the midline of the teeth. the surface of the samples were polished and enamel and dentin were observed under the stereomicroscope.data were analyzed by anova-one way test. the results of this study showed that the least enamel thickness in the central incisor was 345 and in lateral incisor is 235 μ this thickness is related to the one-third labial cervical area. maximum thickness in maxillary central and lateral incisors in the one-third labial incisal surface was 1260 μ and 1220μ, respectively. in the second part of the study, the tendency of dentinal exposure was shown with the chamfer preparation, but no dentinal exposure was found in the knife-edge preparation. the differences between groups were significant (p<0.05).the knowledge of enamel thickness in different part of labial surface is very important. the thickness of enamel in the gingival area does not permit a chamfer preparation. the knife edge preparation is preferable in gingival area.
منابع مشابه
Enamel Thickness After Preparation of Tooth for Porcelain Laminate
OBJECTIVE In this investigation the thickness of enamel in the gingival, middle, and incisal thirds of the labial surface of the anterior teeth were measured regarding preparation of the teeth for porcelain laminate veneers. MATERIALS AND METHODS Part one, 20 extracted intact human maxillary central and lateral incisors ten of each were selected. The teeth were imbedded in autopolimerize acry...
متن کاملPredictable and Precise Tooth Preparation Techniques for Porcelain Laminate Veneers in Complex Cases
Porcelain laminate veneers (PLVs) are one of the most conservative and aesthetic techniques that can be applied when restoring the mouth for improved aesthetics. The longevity of the veneers is good and they are durable, especially if the right indications are in place and the correct techniques are applied (Horn HR, 1983). The fundamental concept in any restorative case is to keep it simple an...
متن کاملIn vitro evaluation of accuracy and precision of automated robotic tooth preparation system for porcelain laminate veneers.
STATEMENT OF PROBLEM Controlling tooth reduction for porcelain laminate veneers (PLVs) in fractions of millimeters is challenging. PURPOSE The purpose of this study was to assess an automated robotic tooth preparation system for PLVs for accuracy and precision compared with conventional freehand tooth preparation. MATERIAL AND METHODS Twenty maxillary central incisor tooth models were divid...
متن کاملEffect of porcelain and enamel thickness on porcelain veneer failure loads in vitro.
STATEMENT OF PROBLEM Bonded porcelain veneers are widely used esthetic restorations. Although high success and survival rates have been reported, failures occur. Fracture is the most common failure mode. Fractures range from incomplete cracks to the catastrophic. Minimally invasive or thin partial veneers have gained popularity. PURPOSE The aim of this study was to measure the influences of p...
متن کاملEffect of Er:YAG Laser Irradiation on Shear Bond Strength of Two Porcelain Laminate Veneers Bonded to Tooth Surface
Background and Aim: The conventional procedure for removal of porcelain laminate veneers (PLVs) is time-consuming and inconvenient. The purpose of this study was to evaluate the efficacy of Er:YAG laser for debonding of PLVs. Materials and Methods: Forty-eight intact extracted human maxillary anterior teeth received discoid PLVs (24 feldspathic and 24 e-max ceramic). The PLVs had 0.7 mm thickn...
متن کاملEffect of tooth substrate and porcelain thickness on porcelain veneer failure loads in vitro.
STATEMENT OF PROBLEM Bonded porcelain veneers are widely used esthetic restorations. High success and survival rates have been reported, but failures do occur. Fractures are the commonest failure mode. Minimally invasive or thin veneers have gained popularity. Increased enamel and porcelain thickness improve the strength of veneers bonded to enamel, but less is known about dentin or mixed subst...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
عنوان ژورنال:
journal of dentistry, tehran university of medical sciencesجلد ۱۱، شماره ۴، صفحات ۴۲۸-۳۲
کلمات کلیدی
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023