this in-vitro study sought to assess the push-out bond strength of a total etch and 2 self-etch bonding systems to intracanal dentin of primary anterior teeth (pat).thirty-six primary anterior teeth were randomly divided into 3 groups of 5(th) generation (single bond 2), 6(th) generation (clearfil se) and 7(th) generation (single bond universal) bonding agents. the canal orifice was restored with composite resin and the push-out test was carried out to assess the bond strength. after applying the push-out load, specimens were evaluated under a light microscope at 40x magnification. one-way anova and log-rank test on kaplan-meier curves were applied for the comparison of bond strength among the 3 groups.the mean± standard deviation (sd) bond strength was 13.6±5.33 mpa for single bond 2, 13.85±5.86 mpa for clearfil se and 12.28±5.24 mpa for single bond universal. the differences in bond strength among the 3 groups were not statistically significant (p>0.05).all three bonding agents are recommended for use with composite posts in pat. however, due to high technical sensitivity of the total etch system, single or two-step self etch systems may be preferred for uncooperative children.
منابع مشابه
Bond Strength of 5th, 6th and 7th Generation Bonding Agents to Intracanal Dentin of Primary Teeth
OBJECTIVES This in-vitro study sought to assess the push-out bond strength of a total etch and 2 self-etch bonding systems to intracanal dentin of primary anterior teeth (PAT). MATERIALS AND METHODS Thirty-six primary anterior teeth were randomly divided into 3 groups of 5(th) generation (Single Bond 2), 6(th) generation (Clearfil SE) and 7(th) generation (Single Bond Universal) bonding agent...
متن کاملComparative Evaluation of Microshear Bond Strength of 5th, 6th and 7th Generation Bonding Agents to Coronal Dentin Versus Dentin at Floor of Pulp Chamber: An In vitro Study
BACKGROUND Lack of seal and adhesion between the final restoration and tooth structure adversely affects the results of root canal treatment. Lots of adhesive bonding agents are marketed to overcome this deficiency and achieve successful restoration. So the study compares and evaluates the micro shear bond strength of coronal dentin and pulp chamber dentin using three different generation denti...
متن کاملIn vitro Comparative Evaluation of Tensile Bond Strength of 6th, 7th and 8th Generation Dentin Bonding Agents
BACKGROUND Newer dentin bonding agents were developed to improve the quality of composite restoration and to reduce time consumption in its application. The aim of the present study was to evaluate tensile bond strength of 6(th), 7(th) and 8(th) generation bonding agents by in vitro method. MATERIALS AND METHODS Selected 60 permanent teeth were assigned into 20 in each group (Group I: 6(th) g...
متن کاملShear bond strength of dentin bonding agents to coronal and radicular dentin
Shear bond strength of dentin bonding agents to coronal and radicular dentin Dr. M. Barakatin * - Dr. MR. Malekypour * - Dr. P. Farjampour ** *Assistant Professor of Operative Dentistry & Dental Materials Dept., Faculty of Dentistry, Azad University (Khorasgan). ** Dentist. Abstract Background and Aim: The purpose of this study was to compare the shear bond strength of three bonding agents know...
متن کاملaffect of age on composite bond strength to dentine using 5th and 6th generation adhesive system
abstract introduction: the mineral content of dentin increases with age and its primary structure is altered. these changes may have unknown effects on efficiency of adhesive systems. the aim of this study was to find the effect of aging on dentin bonding agents. methods and materials: fourty eight extracted human premolars were divided into 2 groups under 15 years old & 2 groups over 45 years ...
متن کاملEffect of Etching Time and Preparation on Push-Out Bond Strength of Composite to Intracanal Dentin of Primary Anterior Teeth
OBJECTIVES This in-vitro study aimed to compare the push-out bond strength of composite to prepared and unprepared intracanal dentin using a 5th generation bonding agent in primary anterior teeth after etching for seven and 15 seconds. MATERIALS AND METHODS Sixty primary anterior teeth were randomly divided into four groups. In groups one and two, intracanal dentin remained intact while in gr...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
عنوان ژورنال:
journal of dentistry, tehran university of medical sciencesجلد ۱۲، شماره ۲، صفحات ۹۰-۸
کلمات کلیدی
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023